Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Pyramid™ KD2250-NT - PEEK-CF30 - Polymics, Ltd.

Material Data Center offers the following functions for Pyramid™ KD2250-NT:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Pyramid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Características de processamento/físicasValorUnidadeMétodo de ensaio
ASTM Dados
Contração após a moldagem, paralelo 0.003 mm/mm ASTM D 955
Propriedades mecânicasValorUnidadeMétodo de ensaio
ASTM Dados
Módulo de tração 23000 MPa ASTM D 638
Resistência à tração 232 MPa ASTM D 638
Deformação na ruptura 2 % ASTM D 638
Resistência à compressão 240 MPa ASTM D 695
Módulo de flexão 21000 MPa ASTM D 790
Dureza Rockwell R 124 - ASTM D 785
Impacto Izod com entalhe, 1/8 in 58.7 J/m ASTM D 256
Propriedades térmicasValorUnidadeMétodo de ensaio
ASTM Dados
UL94 flamabilidade V-0 - UL 94
Coeficiente de expansão térmica, long. 14 E-6/K ASTM D 696
DTUL @ 264 psi 315 °C ASTM D 648
Temperatura de fusão 344 °C ASTM D 3418
Temp. de transição vítrea 143 °C ASTM E 1356
Condutividade térmica, estado sólido 0.133 W/(m K) ASTM C 177
Outras propriedadesValorUnidadeMétodo de ensaio
Absorção de água, 24hr 0.06 % ASTM D 570
Densidade 1400 kg/m³ ASTM D 792
Características
Disponibilidade regional
América do Norte, Europa, Ásia Pacífico
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.