Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Relene E41003 - (PE-HD) - Reliance Polymers

Material Data Center offers the following functions for Relene E41003:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Relene datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Características de processamento/físicasValorUnidadeMétodo de ensaio
ASTM Dados
Índice de fluidez, MFI 1.1 g/10min ASTM D 1238
Temperatura 190 °C -
Carga 5 kg -
Propriedades mecânicasValorUnidadeMétodo de ensaio
ASTM Dados
Resistência à tração 24 MPa ASTM D 638
Resistência à tração no escoamento 20 MPa ASTM D 638
Deformação na ruptura 500 % ASTM D 638
Outras propriedadesValorUnidadeMétodo de ensaio
Densidade 946 kg/m³ ASTM D 792
Características
Processamento
Extrusão de tubos
Características
Resistência de derreta
Certifications
Contacto com alimentos, Aprovação de alimentos FDA 21 CFR
Aplicaciones
Polivalente
Disponibilidade regional
Europa, Ásia Pacífico, Oriente/África
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.