Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Rilsan® BESNO P40 W6 TL - PA11 FR(30) - ARKEMA

Material Data Center offers the following functions for Rilsan® BESNO P40 W6 TL:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Rilsan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto
PA11-P, EFHL, 22-005
Rilsan® BESNO P40 W6 TL resin is a polyamide 11 produced from a renewable source. This grade is plasticized and designed for extrusion.

This grade is classified as Halogen Free Flame Retardant (HFFR).




Main applications:
  • Fluid transportation


Packaging:

This grade is delivered dried in sealed packaging (25 kg bags) ready to be processed.

Shelf Life:
Two years from the delivery. For any use above this limit, please refer to our technical services.
Propriedades mecânicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Módulo de tração - / 540 MPa ISO 527
Tensão no escoamento - / 24 MPa ISO 527
Deformação no escoamento - / 41 % ISO 527
Deformação nominal na ruptura - / >50 % ISO 527
Res. impacto Charpy c/entalhe, +23°C - / 25 kJ/m² ISO 179/1eA
Res. impacto Charpy c/entalhe, -30°C - / 7 kJ/m² ISO 179/1eA
Propriedades térmicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Temperatura de fusão, 10°C/min 180 / * °C ISO 11357-1/-3
Temperatura de deflexão térmica, 1.80 MPa 47 / * °C ISO 75-1/-2
Temperatura de deflexão térmica, 0.45 MPa 130 / * °C ISO 75-1/-2
Flamabilidade a 1.5mm esp. nom. V-2 / * class IEC 60695-11-10
Espessuras do tubo de teste 1.6 / * mm -
Cartão Amarelo (yellow card) disponível sim / * - -
Outras propriedadesSeco / CondUnidadeMétodo de ensaio
Densidade 1110 / 1110 kg/m³ ISO 1183
Biobased content 79 % -
Características
Processamento
Extrusão de perfis, Outros tipos de extrusão
Forma de entrega
Granulos
Aditivos
Plastificante
Características especiais
Retardante de chama, Estável a luz, Estabilidade a raios U.V./Intempéries, Estável contra o calor
Certifications
Contém recursos renováveis
Disponibilidade regional
Outras informações
Outros tipos de extrusão

Processing conditions:

- Typical melt temperature (Min / Recommended / Max) : 210°C / 220°C / 230°C.
- Drying time and temperature (only necessary for bags opened for more than two hours) : 4-8 hours at 80-90°C.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.