Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Rilsan® BMNO P20 TLD - PA11 - ARKEMA

Material Data Center offers the following functions for Rilsan® BMNO P20 TLD:
unit conversion, PDF datasheet print, comparison with other plastics, parameters for material models, CAE Interfaces

Check here, which other Rilsan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto
PA11-P, MHLR, 12-005
Rilsan® BMNO P20 TLD resin is a polyamide 11 produced from a renewable source. This natural grade is plasticized and designed for injection molding.



Main applications:
  • Tennis racquet bumpers

Packaging:
This grade is delivered dried in sealed packaging (25 kg bags) ready to be processed.

Shelf Life:
Two years from the delivery. For any use above this limit, please refer to our technical services.
Características de processamento/físicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez volumétrico, MVR 32 / * cm³/10min ISO 1133
Temperatura 235 / * °C -
Carga 2.16 / * kg -
Contração após a moldagem, paralelo 1.3 / * % ISO 294-4, 2577
Contração após a moldagem, perpendicular 1.4 / * % ISO 294-4, 2577
Propriedades mecânicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Módulo de tração - / 545 MPa ISO 527
Tensão no escoamento - / 32 MPa ISO 527
Deformação no escoamento - / 30 % ISO 527
Deformação nominal na ruptura - / >50 % ISO 527
Res. impacto Charpy c/entalhe, -30°C - / 7 kJ/m² ISO 179/1eA
Dureza Shore D 61 / * - ISO 7619-1
Propriedades térmicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Temperatura de fusão, 10°C/min 186 / * °C ISO 11357-1/-3
Temperatura de deflexão térmica, 1.80 MPa 47 / * °C ISO 75-1/-2
Temperatura de deflexão térmica, 0.45 MPa 135 / * °C ISO 75-1/-2
Temperatura de amolecimento Vicat, B 145 / * °C ISO 306
Coef. de expansão térmica linear, paralelo 100 / * E-6/K ISO 11359-1/-2
Propriedades elétricasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Constante dielétrica, 100Hz 7 / - - IEC 62631-2-1
Constante dielétrica, 1MHz 3 / - - IEC 62631-2-1
Fator de dissipação dielétrica, 100Hz 1900 / - E-4 IEC 62631-2-1
Fator de dissipação dielétrica, 1MHz 614 / - E-4 IEC 62631-2-1
Resistividade volumétrica específica - / 1E10 Ohm*m IEC 62631-3-1
Resistividade superficial específica * / 2E12 Ohm IEC 62631-3-2
Resistência elétrica - / 26 kV/mm IEC 60243-1
Índice comparativo de linha de fuga * / 600 - IEC 60112
Outras propriedadesSeco / CondUnidadeMétodo de ensaio
Absorção de água 1.8 / * % Sim. to ISO 62
Densidade 1050 / 1050 kg/m³ ISO 1183
Biobased content 92 % -
Recomendação de processamento Moldagem por injeçãoValorUnidadeMétodo de ensaio
Pré-secagem - temperatura 80 - 90 °C -
Pré-secagem - tempo 4 - 6 h -
Temperatura da massa 210 - 280 °C -
Temperatura do molde 20 - 60 °C -
Diagrama
Viscosidade - taxa de cisalhamento , Rilsan® BMNO P20 TLD, PA11, ARKEMA
Tensão de cisalhamento - taxa de cisalhamento , Rilsan® BMNO P20 TLD, PA11, ARKEMA
Módulo de cisalhamento dinâmico - temperatura , Rilsan® BMNO P20 TLD (dry), PA11, ARKEMA
Tensão - deformação , Rilsan® BMNO P20 TLD (dry), PA11, ARKEMA
Módulo secante - deformação , Rilsan® BMNO P20 TLD (dry), PA11, ARKEMA
Características
Processamento
Moldagem por injeção
Forma de entrega
Granulos
Aditivos
Desmoldante, Plastificante
Características especiais
Estável a luz, Estabilidade a raios U.V./Intempéries, Estável contra o calor
Certifications
Contém recursos renováveis
Disponibilidade regional
Outras informações
Moldagem por injeção

Processing conditions:

- Typical melt temperature (Min / Recommended / Max) : 210°C / 230°C / 280°C.
- Mold temperature : 20 - 60°C

- Drying time and temperature (only necessary for bags opened for more than two hours) : 4-6 hours at 80-90°C.
Resistência em meio químico
Ácidos
Ácido Acético (5% em massa) (23°C)
Solução de Ácido Cítrico (10% em massa) (23°C)
Ácido Láctico (10% em massa) (23°C)
Ácido Hidroclorídrico (36% em massa) (23°C)
Ácido Nítrico (40% em massa) (23°C)
Ácido Sulfúrico (38% em massa) (23°C)
Ácido Sulfúrico (5% em massa) (23°C)
Solução de Ácido Crômico (40% em massa) (23°C)
Bases
Solução de Hidróxido de Sódio (35% em massa) (23°C)
Solução de Hidróxido de Sódio (1% em massa) (23°C)
Solução de Hidróxido de Amônio (10% em massa) (23°C)
Álcoois
Metanol (23°C)
Etanol (23°C)
Hidrocarbonetos
n-Hexano (23°C)
Tolueno (23°C)
Cetonas
Acetona (23°C)
Óleos Minerais
Óleo de motor multissérie SAE 10W40 (23°C)
Óleo de motor multissérie SAE 10W40 (130°C)
Óleo de engrenagem hipóide SAE 80/90 (130°C)
Óleo isolante (23°C)
Combustíveis Padrões
Líquido 1 ISO 1817 (60°C)
Líquido 2 ISO 1817 (60°C)
Líquido 3 ISO 1817 (60°C)
Líquido 4 ISO 1817 (60°C)
Combustível padrão sem álcool (pref. Líquico C ISO 1817) (23°C)
Combustível padrão com álcool (pref. Líquico 4 ISO 1817) (23°C)
Diesel (pref. Líquido F ISO 1817) (23°C)
Diesel (pref. Líquido F ISO 1817) (90°C)
Diesel (pref. Líquido F ISO 1817) (>90°C)
Soluções de sais
Solução de Cloreto de Sódio (10% em massa) (23°C)
Solução de Hipoclorito de Sódio (10% em massa) (23°C)
Solução de Cloreto de Zinco (50% em massa) (23°C)
Outras
Acetato de Etila (23°C)
Peróxido de Hidrogênio (23°C)
Fluido de freio DOT No. 4 (130°C)
Etileno Glicol (50% em massa) em água (108°C)
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.