Material datasheets available free. Online registration at: www.materialdatacenter.com
Skypel - TPE - SK Chemicals
Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "Skypel" in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
Datasheet | Polymer |
---|---|
SKYPEL G130D | TPE |
SKYPEL G140D | TPE |
SKYPEL G155D | TPE |
SKYPEL G163D | TPE |
SKYPEL G172D | TPE |
SKYPEL G182D | TPE |
SKYPEL P128DF | TPE |
SKYPEL P137DF | TPE |
SKYPEL P147DF | TPE |
SKYPEL P155DF | TPE |
SKYPEL G240D | TPE |
SKYPEL G940DW | TPE |
SKYPEL P142DF | TPE |
SKYPEL G140DW | TPE |
SKYPEL LP380A | TPE |
SKYPEL LX770A | TPE |
SKYPEL LX780A | TPE |
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.