Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of STYRON™ 636 BT - PS - Trinseo

Material Data Center offers the following functions for STYRON™ 636 BT:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Styron datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Características de processamento/físicasValorUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez, MFI 3.1 g/10min ISO 1133
Temperatura 200 °C -
Carga 5 kg -
Propriedades mecânicasValorUnidadeMétodo de ensaio
ISO Dados
Tensão no escoamento 55 MPa ISO 527
Deformação na ruptura 2 % ISO 527
Módulo de flexão, 23°C 3500 MPa ISO 178
Resistência à flexão 80 MPa ISO 178
Dureza Rockwell R 105 - ISO 2039-2
Ball indentation hardness 150 MPa ISO 2039-1
Propriedades térmicasValorUnidadeMétodo de ensaio
ISO Dados
Temperatura de deflexão térmica, 1.80 MPa 90[ann.] °C ISO 75-1/-2
Temperatura de deflexão térmica , 0.45 MPa 93[ann.] °C ISO 75-1/-2
Temperatura de amolecimento Vicat , A 96.5 °C ISO 306
Flamabilidade a 1.5mm esp. nom. HB class IEC 60695-11-10
Espessuras do tubo de teste 1.6 mm -
ann.: annealed
Propriedades elétricasValorUnidadeMétodo de ensaio
ASTM Dados
Fator de dissipação dielétrica, 1 MHz 6.0E-5 - ASTM D 150
Constante dielétrica, 1 MHz 2.5 - ASTM D 150
Outras propriedadesValorUnidadeMétodo de ensaio
Densidade 1050 kg/m³ ISO 1183
Bulk density 600 kg/m³ -
Características
Processamento
Moldagem por injeção, Outros tipos de extrusão, Termoformagem
Características
Mistura de resina, Foamable
Certifications
Contacto com alimentos, Aprovação para contacto com alimentos10/2011, Aprovação de alimentos FDA 21 CFR
Aplicaciones
Polivalente, Embalaje, Refrigeración
Disponibilidade regional
Europa, Oriente/África
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.