Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of STYRON™ 686 E - PS - Trinseo

Material Data Center offers the following functions for STYRON™ 686 E:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Styron datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Características de processamento/físicasValorUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez, MFI 2.5 g/10min ISO 1133
Temperatura 200 °C -
Carga 5 kg -
ASTM Dados
Índice de fluidez, MFI 2.5 g/10min ASTM D 1238
Temperatura 200 °C -
Carga 5 kg -
Propriedades mecânicasValorUnidadeMétodo de ensaio
ISO Dados
Tensão no escoamento 55 MPa ISO 527
Deformação na ruptura 2 % ISO 527
Módulo de flexão, 23°C 3600 MPa ISO 178
Dureza Rockwell R105 - ISO 2039-2
ASTM Dados
Resistência à tração no escoamento 55 MPa ASTM D 638
Deformação na ruptura 2 % ASTM D 638
Módulo de flexão 3599 MPa ASTM D 790
Resistência à flexão 90.3 MPa ASTM D 790
Propriedades térmicasValorUnidadeMétodo de ensaio
ISO Dados
Temperatura de amolecimento Vicat , A 107 °C ISO 306
Temperatura de amolecimento Vicat, B 100 °C ISO 306
Coef. de expansão térmica linear, paralelo 80 E-6/K ISO 11359-1/-2
Flamabilidade a 1.5mm esp. nom. HB class IEC 60695-11-10
Espessuras do tubo de teste 1.6 mm -
ASTM Dados
UL94 flamabilidade HB - UL 94
Espessuras do tubo de teste 1.6 mm -
Propriedades elétricasValorUnidadeMétodo de ensaio
ISO Dados
Resistência elétrica 140 kV/mm IEC 60243-1
ASTM Dados
Fator de dissipação dielétrica, 1 MHz 6.0E-5 - ASTM D 150
Constante dielétrica, 1 MHz 2.5 - ASTM D 150
Outras propriedadesValorUnidadeMétodo de ensaio
Densidade 1050 kg/m³ ISO 1183
Densidade 1050 kg/m³ ASTM D 792
Características
Processamento
Moldagem por injeção, Outros tipos de extrusão
Características especiais
Estável contra o calor
Características
Foamable
Certifications
Contacto com alimentos, Aprovação para contacto com alimentos10/2011, Aprovação de alimentos FDA 21 CFR
Aplicaciones
Polivalente, Embalaje
Disponibilidade regional
Europa, Oriente/África
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com