Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of TORZEN G5000HSL BK20 - PA66-GF50 - RadiciGroup High Performance Polymers

Material Data Center offers the following functions for TORZEN G5000HSL BK20:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Torzen datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto
PA66 50% glass fibre reinforced injection moulding grade. Heat stabilized. Black colour.

Suitable for parts requiring very high stiffness and mechanical resistance, along with good heat ageing properties retention.
Características de processamento/físicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Contração após a moldagem, paralelo 0.2 / * % ISO 294-4, 2577
Contração após a moldagem, perpendicular 0.9 / * % ISO 294-4, 2577
Propriedades mecânicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 16500 / 12000 MPa ISO 527
Tensão na ruptura 245 / 170 MPa ISO 527
Deformação na ruptura 2.5 / 3 % ISO 527
Resistência ao impacto Charpy , +23°C 95 / 105 kJ/m² ISO 179/1eU
Resistência ao impacto Charpy, -30°C 90 / - kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalhe, +23°C 17 / 22 kJ/m² ISO 179/1eA
Res. impacto Charpy c/entalhe, -30°C 15 / - kJ/m² ISO 179/1eA
Propriedades térmicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Temperatura de fusão, 10°C/min 260 / * °C ISO 11357-1/-3
Temperatura de deflexão térmica, 1.80 MPa 255 / * °C ISO 75-1/-2
Temperatura de deflexão térmica, 0.45 MPa 260 / * °C ISO 75-1/-2
Flamabilidade a espessura h HB / * class IEC 60695-11-10
Espessuras do tubo de teste 0.4 / * mm -
Cartão Amarelo (yellow card) disponível sim / * - -
Outras propriedadesSeco / CondUnidadeMétodo de ensaio
Absorção de umidade 1.1 / * % Sim. to ISO 62
Densidade 1580 / - kg/m³ ISO 1183
Características
Processamento
Moldagem por injeção
Forma de entrega
Granulado, Negro
Aditivos
Desmoldante
Características especiais
Estável contra o calor
Disponibilidade regional
Outras informações
Moldagem por injeção
The material is delivered in moisture-proof packaging ready for processing. Maximum recommended water content for best processing is 0.15%. Typical conditions with a desiccant drier: temperature 80 ° C, dew point -20 ° C or below, time 2-4 h or more. Special care must be taken to avoid moisture absorption and contamination with other polymers when adding regrind material. Colour variation and mechanical properties reduction may occur and should always be carefully monitored.

Injection Molding Processing Parameters
Melt TemperatureMold TemperatureInjection Speed
280 - 300°C80 - 100°Cmedium-high
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com