Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultradur® B 4520 FC R01 - PBT - BASF

Material Data Center offers the following functions for Ultradur® B 4520 FC R01:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Ultradur datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto
Ultradur® B4520 FC R01 UN is suitable for plastic parts, where material approval direct food contact is a mandatory requirement.

The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulations including European Food Contact (EU) Nr. 10/2011 and GMP (EC) N°2023/2006.

For questions regarding the compliance with further regulations, and certificates, please contact your local BASF representative or Plastics Safety (E-Mail: plastics.safety@basf.com).

The products can also be offered as BMBcert™ and/or Ccycled™. Due to the Massbalance approach the product properties do not change.
Características de processamento/físicasValorUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez volumétrico, MVR 24 cm³/10min ISO 1133
Temperatura 250 °C -
Carga 2.16 kg -
Propriedades mecânicasValorUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 2500 MPa ISO 527
Tensão no escoamento 56 MPa ISO 527
Deformação no escoamento 3.6 % ISO 527
Deformação nominal na ruptura >50 % ISO 527
Resistência ao impacto Charpy , +23°C 260 kJ/m² ISO 179/1eU
Resistência ao impacto Charpy, -30°C 200 kJ/m² ISO 179/1eU
Type of failure C - -
Res. impacto Charpy c/entalhe, +23°C 3.5 kJ/m² ISO 179/1eA
Type of failure C - -
Res. impacto Charpy c/entalhe, -30°C 3 kJ/m² ISO 179/1eA
Propriedades térmicasValorUnidadeMétodo de ensaio
ISO Dados
Temperatura de fusão, 10°C/min 223 °C ISO 11357-1/-3
Temperatura de deflexão térmica, 0.45 MPa 130 °C ISO 75-1/-2
Outras propriedadesValorUnidadeMétodo de ensaio
Densidade 1300 kg/m³ ISO 1183
Propriedades específicas do materialValorUnidadeMétodo de ensaio
ISO Dados
Índice de viscosidade 120 cm³/g ISO 307, 1157, 1628
Características
Certifications
Contacto com alimentos, Aprovação para contacto com alimentos10/2011, Aprovação de alimentos FDA 21 CFR
Outras informações
Moldagem por injeção
PREPROCESSING
Pre/Post-processing, max. allowed water content: .04 %
Pre/Post-processing, Pre-drying, Temperature: 80 - 120 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 250 - 275 °C
injection molding, Melt temperature, recommended: 260 °C
injection molding, Mold temperature, range: 40 - 70 °C
injection molding, Mold temperature, recommended: 60 °C
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com