Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultrafuse PA - PA666 - BASF

Material Data Center offers the following functions for Ultrafuse PA:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ultrafuse datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Características de processamento/físicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez volumétrico, MVR 49.5 / * cm³/10min ISO 1133
Temperatura 275 / * °C -
Carga 5 / * kg -
Propriedades térmicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Temperatura de fusão, 10°C/min 196 / * °C ISO 11357-1/-3
Temp. de transição vítrea, 10 °C/min 49 / * °C ISO 11357-1/-2
Temperatura de deflexão térmica, 1.80 MPa 65 / * °C ISO 75-1/-2
Temperatura de deflexão térmica , 0.45 MPa 135 / * °C ISO 75-1/-2
Temperatura de amolecimento Vicat, B 172 / * °C ISO 306
Outras propriedadesSeco / CondUnidadeMétodo de ensaio
Densidade 1110 / 1050 kg/m³ ISO 1183
3D DataSeco / CondUnidadeMétodo de ensaio
Other Standards[S]
Módulo de tração, flat 2420 / 395 MPa ISO 527
Módulo de tração, upright 2120 / 334 MPa ISO 527
Resistência à tração, flat 61.4 / 33.2 MPa ISO 527
Resistência à tração, upright 16.4 / 17.6 MPa ISO 527
Deformação na ruptura, flat 9.6 / 143 % ISO 527
Deformação na ruptura, upright 0.8 / 12.8 % ISO 527
Módulo de flexão, flat 2050 / 445 MPa ISO 178
Módulo de flexão, on-edge 2250 / 468 MPa ISO 178
Módulo de flexão, upright 2150 / 428 MPa ISO 178
Resistência à flexão, flat 77 / 17.7 MPa ISO 178
Resistência à flexão, on-edge 95.5 / 18.1 MPa ISO 178
Resistência à flexão, upright 40.2 / 17.3 MPa ISO 178
Resistência ao impacto Charpy, +23°C, flat 23 / 0 kJ/m² ISO 179/1eU
Resistência ao impacto Charpy, +23°C, on-edge 29.7 / 0 kJ/m² ISO 179/1eU
Resistência ao impacto Charpy, +23°C, upright 3.5 / 13.4 kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalhe, +23°C, flat 5.6 / - kJ/m² ISO 179/1eA
Res. impacto Charpy c/entalhe, +23°C, on-edge 3.3 / 136 kJ/m² ISO 179/1eA
Res. impacto Charpy c/entalhe, +23°C, upright 1.2 / 9.4 kJ/m² ISO 179/1eA
Resistência ao Impacto Izod, +23°C, flat 28 / 0 kJ/m² ISO 180/1U
Resistência ao Impacto Izod, +23°C, on-edge 45.6 / 0 kJ/m² ISO 180/1U
Resistência ao Impacto Izod, +23°C, upright 3.2 / 17.4 kJ/m² ISO 180/1U
Impacto Izod com entalhe, +23°C, flat 5.8 / 85.4 kJ/m² ISO 180/1A
Impacto Izod com entalhe, +23°C, on-edge 3.9 / 106 kJ/m² ISO 180/1A
Impacto Izod com entalhe, +23°C, upright 1.7 / 10.1 kJ/m² ISO 180/1A
S: These properties are reported by the producer according standards that are different to our defaults.
Características
Processamento
Additive Manufacturing
Forma de entrega
Monofilament
Características
Estabilidade térmica
Disponibilidade regional
América do Norte, Europa, America Centra e do Sul
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.