Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultrafuse PPSU - PPSU - BASF

Material Data Center offers the following functions for Ultrafuse PPSU:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ultrafuse datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Características de processamento/físicasValorUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez volumétrico, MVR 39 cm³/10min ISO 1133
Temperatura 360 °C -
Carga 10 kg -
Propriedades térmicasValorUnidadeMétodo de ensaio
ISO Dados
Temp. de transição vítrea, 10 °C/min 220 °C ISO 11357-1/-2
Temperatura de deflexão térmica, 1.80 MPa 212 °C ISO 75-1/-2
Temperatura de deflexão térmica , 0.45 MPa 218 °C ISO 75-1/-2
Temperatura de amolecimento Vicat, B 220 °C ISO 306
Coef. de expansão térmica linear, paralelo 55 E-6/K ISO 11359-1/-2
Outras propriedadesValorUnidadeMétodo de ensaio
Densidade 1210 kg/m³ ISO 1183
3D DataValorUnidadeMétodo de ensaio
Other Standards[S]
Módulo de tração, flat 2040 MPa ISO 527
Módulo de tração, upright 2040 MPa ISO 527
Resistência à tração, flat 65.1 MPa ISO 527
Resistência à tração, upright 51.6 MPa ISO 527
Deformação na ruptura, flat 6.5 % ISO 527
Deformação na ruptura, upright 3.2 % ISO 527
Módulo de flexão, flat 2150 MPa ISO 178
Módulo de flexão, upright 2000 MPa ISO 178
Resistência à flexão, flat 92.6 MPa ISO 178
Resistência à flexão, upright 96.5 MPa ISO 178
Resistência ao impacto Charpy, +23°C, flat 201 kJ/m² ISO 179/1eU
Resistência ao impacto Charpy, +23°C, upright 22.6 kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalhe, +23°C, flat 13.8 kJ/m² ISO 179/1eA
Res. impacto Charpy c/entalhe, +23°C, upright 5.5 kJ/m² ISO 179/1eA
Resistência ao Impacto Izod, +23°C, flat 119 kJ/m² ISO 180/1U
Resistência ao Impacto Izod, +23°C, upright 14.3 kJ/m² ISO 180/1U
Impacto Izod com entalhe, +23°C, flat 12 kJ/m² ISO 180/1A
Impacto Izod com entalhe, +23°C, upright 5.5 kJ/m² ISO 180/1A
S: These properties are reported by the producer according standards that are different to our defaults.
Características
Processamento
Additive Manufacturing
Forma de entrega
Monofilament
Características
Boa adesão, Estabilidade térmica
Resistência Química
Resistência química geral
Disponibilidade regional
América do Norte, Europa, America Centra e do Sul
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.