Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAKEEP® 3300 G - PEEK - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAKEEP® 3300 G:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestakeep datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto
Medium-viscosity, unreinforced polyether ether ketone

VESTAKEEP® 3300 G is a medium-viscosity, unreinforced polyether ether ketone for injection molding and extrusion.

The semi-crystalline polymer features superior thermal and chemical resistance. Parts made from VESTAKEEP® 3300G are of low flammability.

VESTAKEEP® 3300 G can be processed by common machines for thermoplastics.

We recommend a melt temperature between 360°C and 380°C during the injection molding process. The mold temperature should be within a range of 160°C to 200°C, preferably 180°C.

VESTAKEEP® 3300 G is supplied as granules in 25 kg boxes with moisture-proof poly­ethylene liners.

Pigmentation may affect values.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing VESTAKEEP® 3300 G, please follow the general recommendations in our brochure “VESTAKEEP® PEEK Processing Guidelines".

The values presented are typical or average values, they do not constitute a specification. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM OR VISIT OUR PRODUCT AT  WWW.INDUSTRIAL.VESTAKEEP.COM
Características de processamento/físicasValorUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez volumétrico, MVR 20 cm³/10min ISO 1133
Temperatura 380 °C -
Carga 5 kg -
Contração após a moldagem, paralelo 0.9 % ISO 294-4, 2577
Contração após a moldagem, perpendicular 1.1 % ISO 294-4, 2577
Propriedades mecânicasValorUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 3600 MPa ISO 527
Tensão no escoamento 95 MPa ISO 527
Deformação no escoamento 5 % ISO 527
Deformação nominal na ruptura 25 % ISO 527
Resistência ao impacto Charpy , +23°C N kJ/m² ISO 179/1eU
Resistência ao impacto Charpy, -30°C N kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalhe, +23°C 7 kJ/m² ISO 179/1eA
Type of failure C - -
Res. impacto Charpy c/entalhe, -30°C 6 kJ/m² ISO 179/1eA
Type of failure C - -
Propriedades térmicasValorUnidadeMétodo de ensaio
ISO Dados
Temperatura de fusão, 10°C/min 340 °C ISO 11357-1/-3
Temp. de transição vítrea, 10°C/min 152 °C ISO 11357-1/-2
Temperatura de deflexão térmica, 1.80 MPa 155 °C ISO 75-1/-2
Temperatura de deflexão térmica, 0.45 MPa 205 °C ISO 75-1/-2
Temperatura de amolecimento Vicat, B 305 °C ISO 306
Coef. de expansão térmica linear, paralelo 60 E-6/K ISO 11359-1/-2
Cartão Amarelo (yellow card) disponível sim - -
Flamabilidade conforme índice de oxigênio 38 % ISO 4589-1/-2
Propriedades elétricasValorUnidadeMétodo de ensaio
ISO Dados
Constante dielétrica, 100Hz 2.8 - IEC 62631-2-1
Constante dielétrica, 1MHz 2.8 - IEC 62631-2-1
Fator de dissipação dielétrica, 100Hz 30 E-4 IEC 62631-2-1
Fator de dissipação dielétrica, 1MHz 50 E-4 IEC 62631-2-1
Resistividade volumétrica específica >1E13 Ohm*m IEC 62631-3-1
Resistividade superficial específica 1E15 Ohm IEC 62631-3-2
Resistência elétrica 33.9 kV/mm IEC 60243-1
Índice comparativo de linha de fuga 200 - IEC 60112
Outras propriedadesValorUnidadeMétodo de ensaio
Absorção de água 0.5 % Sim. to ISO 62
Densidade 1300 kg/m³ ISO 1183
Produção de amostra para testeValorUnidadeMétodo de ensaio
ISO Dados
Moldagem por injeção, temperatura da massa 380 °C ISO 294
Moldagem por injeção, temperatura do molde 180 °C ISO 294
Moldagem por injeção, velocidade de injeção 200 mm/s ISO 294
Moldagem por injeção, pressão de recalque 120 MPa ISO 294
Características
Processamento
Moldagem por injeção, Extrusão de laminas, Extrusão de perfis, Outros tipos de extrusão
Forma de entrega
Granulos
Resistência Química
Resistência química geral
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.