Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAKEEP® 4000 CF30 - PEEK-CF30 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAKEEP® 4000 CF30:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestakeep datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto
Carbon fiber-reinforced (30%), high viscosity polyether ether ketone

VESTAKEEP® 4000 CF30 is a carbon fiber reinforced (30%) polyether ether ketone for injection molding.

The semi-crystalline polymer features superior mechanical, thermal, and chemical resistance. Parts made from VESTAKEEP® 4000 CF30 are of low flammability.

VESTAKEEP® 4000 CF30 can be processed by common injection molding machines for thermoplastics.

We recommend a melt temperature between 380°C and 400°C during the injection molding process. The mold temperature should be within a range of 160°C to 200°C, preferably 180°C.

VESTAKEEP® 4000 CF30 is supplied as granules in 25 kg boxes with moisture-proof polyethylene liners.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

Pigmentation may affect values.

For information about processing VESTAKEEP® 4000 CF30, please follow the general recommendations in our brochure “VESTAKEEP® PEEK Processing Guidelines.“

The values presented are typical or average values, they do not constitute a specification. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM OR VISIT OUR PRODUCT AT WWW.INDUSTRIAL.VESTAKEEP.COM
Características de processamento/físicasValorUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez volumétrico, MVR 20 cm³/10min ISO 1133
Temperatura 380 °C -
Carga 21.6 kg -
Contração após a moldagem, paralelo 0 % ISO 294-4, 2577
Contração após a moldagem, perpendicular 0.4 % ISO 294-4, 2577
Propriedades mecânicasValorUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 23000 MPa ISO 527
Tensão na ruptura 240 MPa ISO 527
Deformação na ruptura 2 % ISO 527
Resistência ao impacto Charpy , +23°C 60 kJ/m² ISO 179/1eU
Type of failure C - -
Resistência ao impacto Charpy, -30°C 60 kJ/m² ISO 179/1eU
Type of failure C - -
Res. impacto Charpy c/entalhe, +23°C 10 kJ/m² ISO 179/1eA
Type of failure C - -
Res. impacto Charpy c/entalhe, -30°C 9 kJ/m² ISO 179/1eA
Type of failure C - -
Propriedades térmicasValorUnidadeMétodo de ensaio
ISO Dados
Temperatura de fusão, 10°C/min 340 °C ISO 11357-1/-3
Temperatura de deflexão térmica, 1.80 MPa 325 °C ISO 75-1/-2
Temperatura de deflexão térmica, 0.45 MPa 335 °C ISO 75-1/-2
Temperatura de amolecimento Vicat, B 340 °C ISO 306
Coef. de expansão térmica linear, paralelo 10 E-6/K ISO 11359-1/-2
Flamabilidade a 1.5mm esp. nom. V-0 class IEC 60695-11-10
Espessuras do tubo de teste 1.6 mm -
Flamabilidade a espessura h V-0 class IEC 60695-11-10
Espessuras do tubo de teste 0.8 mm -
Flamabilidade conforme índice de oxigênio 47 % ISO 4589-1/-2
Propriedades elétricasValorUnidadeMétodo de ensaio
ISO Dados
Constante dielétrica, 1MHz 17 - IEC 62631-2-1
Fator de dissipação dielétrica, 1MHz 230 E-4 IEC 62631-2-1
Resistividade volumétrica específica 10000 Ohm*m IEC 62631-3-1
Resistividade superficial específica 1000000 Ohm IEC 62631-3-2
Outras propriedadesValorUnidadeMétodo de ensaio
Absorção de água 0.4 % Sim. to ISO 62
Densidade 1400 kg/m³ ISO 1183
Produção de amostra para testeValorUnidadeMétodo de ensaio
ISO Dados
Moldagem por injeção, temperatura da massa 420 °C ISO 294
Moldagem por injeção, temperatura do molde 200 °C ISO 294
Moldagem por injeção, velocidade de injeção 200 mm/s ISO 294
Moldagem por injeção, pressão de recalque 120 MPa ISO 294
Diagrama
Módulo de tração - temperatura , VESTAKEEP® 4000 CF30, PEEK-CF30, Evonik
Características
Processamento
Moldagem por injeção, Outros tipos de extrusão
Forma de entrega
Granulos
Disponibilidade regional
América do Norte, Europa, Ásia Pacífico, America Centra e do Sul, Oriente/África
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.