Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® Care ML-GB30 - PA12-GB30 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® Care ML-GB30:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto

Microglass bead-filled (30%) PA12 resin for the injection moulding of rigid, low-warpage and dimensionally accurate mouldings

 

Biocompatibility of VESTAMID® Care
VESTAMID® Care ML grades were tested on biocompatibility for applications within the body of up to 30 days contact time and comply with USP <88> class VI and ISO 10993 standards.

Biocompatibility tests for VESTAMID® Care:
Standard Description
ASTM F756-08 Hemocompatibility
ISO 10993-5 Cytotoxicity
ISO 10993-10 Sensitization: Maximization test according to Magnusson and Kligman
ISO 10993-10 Irritation: Intracutaneous Reactivity
ISO 10993-11 Acute Systemic Toxicity
USP Class VI Acute Systemic Toxicity Intracutaneous Reactivity Muscle Implantation
 
Processing of VESTAMID® Care
For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 



FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.EVONIK.COM/MEDICAL-TECHNOLOGY


 

Características de processamento/físicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez volumétrico, MVR 100 / * cm³/10min ISO 1133
Temperatura 275 / * °C -
Carga 5 / * kg -
Contração após a moldagem, paralelo 0.6 / * % ISO 294-4, 2577
Contração após a moldagem, perpendicular 0.7 / * % ISO 294-4, 2577
Propriedades mecânicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 2100 / 1800 MPa ISO 527
Tensão no escoamento 47 / 37 MPa ISO 527
Deformação no escoamento 5 / 5 % ISO 527
Deformação nominal na ruptura 20 / >50 % ISO 527
Módulo de tensão de fluência, 1h * / 1600 MPa ISO 899-1
Módulo de tensão de fluência, 1000h * / 1100 MPa ISO 899-1
Resistência ao impacto Charpy , +23°C 160 / N kJ/m² ISO 179/1eU
Type of failure C / - - -
Resistência ao impacto Charpy, -30°C 160 / N kJ/m² ISO 179/1eU
Type of failure C / - - -
Res. impacto Charpy c/entalhe, +23°C 4.4 / 6 kJ/m² ISO 179/1eA
Type of failure C / C - -
Res. impacto Charpy c/entalhe, -30°C 6 / 6 kJ/m² ISO 179/1eA
Type of failure C / C - -
Propriedades térmicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Temperatura de fusão, 10°C/min 178 / * °C ISO 11357-1/-3
Temperatura de deflexão térmica, 1.80 MPa 55 / * °C ISO 75-1/-2
Temperatura de deflexão térmica, 0.45 MPa 150 / * °C ISO 75-1/-2
Temperatura de amolecimento Vicat, B 155 / * °C ISO 306
Coef. de expansão térmica linear, paralelo 130 / * E-6/K ISO 11359-1/-2
Coef. de expansão térmica linear, perpend. 130 / * E-6/K ISO 11359-1/-2
Flamabilidade a 1.5mm esp. nom. HB / * class IEC 60695-11-10
Espessuras do tubo de teste 1.6 / * mm -
Propriedades elétricasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Constante dielétrica, 100Hz 4.1 / 5 - IEC 62631-2-1
Constante dielétrica, 1MHz 3.5 / 4 - IEC 62631-2-1
Fator de dissipação dielétrica, 100Hz 310 / 600 E-4 IEC 62631-2-1
Fator de dissipação dielétrica, 1MHz 230 / 370 E-4 IEC 62631-2-1
Resistividade volumétrica específica >1E13 / 2E12 Ohm*m IEC 62631-3-1
Resistividade superficial específica * / 1E15 Ohm IEC 62631-3-2
Resistência elétrica - / 36 kV/mm IEC 60243-1
Índice comparativo de linha de fuga 600 / 600 - IEC 60112
Outras propriedadesSeco / CondUnidadeMétodo de ensaio
Absorção de água 1.1 / * % Sim. to ISO 62
Absorção de umidade 0.5 / * % Sim. to ISO 62
Densidade 1250 / 1260 kg/m³ ISO 1183
Diagrama
Viscosidade - taxa de cisalhamento , VESTAMID® Care ML-GB30, PA12-GB30, Evonik
Tensão de cisalhamento - taxa de cisalhamento , VESTAMID® Care ML-GB30, PA12-GB30, Evonik
Módulo de cisalhamento dinâmico - temperatura , VESTAMID® Care ML-GB30 (dry), PA12-GB30, Evonik
Tensão - deformação , VESTAMID® Care ML-GB30 (dry), PA12-GB30, Evonik
Módulo secante - deformação , VESTAMID® Care ML-GB30 (dry), PA12-GB30, Evonik
Tensão - deformação (isocrônico) 23°C, VESTAMID® Care ML-GB30 (cond.), PA12-GB30, Evonik
Módulo de fluência - tempo 23°C, VESTAMID® Care ML-GB30 (cond.), PA12-GB30, Evonik
Curva de fluencia 23°C, VESTAMID® Care ML-GB30 (cond.), PA12-GB30, Evonik
Características
Processamento
Moldagem por injeção
Forma de entrega
Granulos
Características
Baixa deformação
Certifications
Grau médico, Biocompatibility ISO 10993, USP Class VI
Aplicaciones
Médico
Disponibilidade regional
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com