Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® L-GF30 - PA12-GF30 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® L-GF30:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto

Glass fiber-reinforced and heat stabilized polyamide 12

VESTAMID® L-GF30 NC 
is a glass fiber –reinforced heat stabilized Polyamide 12 for injection molding. The material contains about 30% glass fibers, an ageing protective agent and a processing aid for a fast and even form filling. Due to the reinforcement moldings from this compound exhibit a higher strength and  good heat resistance.

Further advantages of VESTAMID® L-GF30 NC are the characterizing properties of PA12, e.g., low water absorption, good dimensional stability and nearly constant mechanical properties at changing ambient humidity.
  
VESTAMID® L-GF30 NC is supplied as cylindrical granules, ready for processing, in moisture-proof bags.
 
Pigmentation may affect values.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM

Características de processamento/físicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez volumétrico, MVR 30 / * cm³/10min ISO 1133
Temperatura 275 / * °C -
Carga 5 / * kg -
Contração após a moldagem, paralelo 0.1 / * % ISO 294-4, 2577
Contração após a moldagem, perpendicular 0.7 / * % ISO 294-4, 2577
Propriedades mecânicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 6800 / 5500 MPa ISO 527
Tensão no escoamento 120 / 110 MPa ISO 527
Deformação no escoamento 5 / 5 % ISO 527
Deformação nominal na ruptura 6 / 5.5 % ISO 527
Resistência ao impacto Charpy , +23°C 93 / 75 kJ/m² ISO 179/1eU
Type of failure C / C - -
Resistência ao impacto Charpy, -30°C 100 / 95 kJ/m² ISO 179/1eU
Type of failure C / C - -
Res. impacto Charpy c/entalhe, +23°C 27 / 24 kJ/m² ISO 179/1eA
Type of failure - / C - -
Res. impacto Charpy c/entalhe, -30°C 21 / 22 kJ/m² ISO 179/1eA
Type of failure C / C - -
Dureza Shore D 79 / * - ISO 7619-1
Propriedades térmicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Temperatura de fusão, 10°C/min 178 / * °C ISO 11357-1/-3
Temp. de transição vítrea, 10°C/min 42 / * °C ISO 11357-1/-2
Temperatura de deflexão térmica, 1.80 MPa 165 / * °C ISO 75-1/-2
Temperatura de deflexão térmica, 0.45 MPa 175 / * °C ISO 75-1/-2
Temperatura de amolecimento Vicat, B 175 / * °C ISO 306
Coef. de expansão térmica linear, paralelo 60 / * E-6/K ISO 11359-1/-2
Flamabilidade a 1.5mm esp. nom. HB / * class IEC 60695-11-10
Espessuras do tubo de teste 1.5 / * mm -
Cartão Amarelo (yellow card) disponível sim / * - -
Flamabilidade a espessura h HB / * class IEC 60695-11-10
Espessuras do tubo de teste 0.8 / * mm -
Cartão Amarelo (yellow card) disponível sim / * - -
Propriedades elétricasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Constante dielétrica, 100Hz 4.1 / 5 - IEC 62631-2-1
Constante dielétrica, 1MHz 3.4 / 4 - IEC 62631-2-1
Fator de dissipação dielétrica, 100Hz 310 / 600 E-4 IEC 62631-2-1
Fator de dissipação dielétrica, 1MHz 330 / 400 E-4 IEC 62631-2-1
Resistividade volumétrica específica >1E13 / 2E12 Ohm*m IEC 62631-3-1
Resistividade superficial específica * / >1E15 Ohm IEC 62631-3-2
Resistência elétrica - / 45 kV/mm IEC 60243-1
Índice comparativo de linha de fuga 600 / 600 - IEC 60112
Outras propriedadesSeco / CondUnidadeMétodo de ensaio
Absorção de água 1.1 / * % Sim. to ISO 62
Absorção de umidade 0.5 / * % Sim. to ISO 62
Densidade 1240 / 1240 kg/m³ ISO 1183
Diagrama
Viscosidade - taxa de cisalhamento , VESTAMID® L-GF30, PA12-GF30, Evonik
Tensão de cisalhamento - taxa de cisalhamento , VESTAMID® L-GF30, PA12-GF30, Evonik
Módulo de cisalhamento dinâmico - temperatura , VESTAMID® L-GF30 (dry), PA12-GF30, Evonik
Tensão - deformação , VESTAMID® L-GF30 (dry), PA12-GF30, Evonik
Módulo secante - deformação , VESTAMID® L-GF30 (dry), PA12-GF30, Evonik
Tensão-deformação (Anisotropia) , VESTAMID® L-GF30 (dry), PA12-GF30, Evonik
Tensão - deformação (isocrônico) 23°C, VESTAMID® L-GF30 (cond.), PA12-GF30, Evonik
Módulo de fluência - tempo 23°C, VESTAMID® L-GF30 (cond.), PA12-GF30, Evonik
Curva de fluencia 23°C, VESTAMID® L-GF30 (cond.), PA12-GF30, Evonik
Módulo de tração - temperatura , VESTAMID® L-GF30 (dry), PA12-GF30, Evonik
Características
Processamento
Moldagem por injeção
Forma de entrega
Granulos, Cor natural
Aditivos
Lubrificantes
Características especiais
Estável contra o calor
Disponibilidade regional
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.