Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® L1670 BK 9.7504 - PA12 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® L1670 BK 9.7504:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto
Low viscosity, heat and light stabilized Polyamide 12 compound

VESTAMID® L1670 BK 9.7504 has been developed especially for the extrusion of thin wire insulations and cable jacketings.
 
VESTAMID® L1670 BK 9.7504 coatings exhibit a low coefficient of friction which facilitates the laying of cable.
 
Switchboard wiring isolated with VESTAMID® L1670 BK 9.7504 can be soldered with no worry of interference by the plastic resin. The wiring can be soldered without the need to strip the isolating layer.
 
Jacketing of VESTAMID® L1670 BK 9.7504 protects buried cables from attack by termites.
 

This partially crystalline polyamide 12 bases compounds have a very low water ab­sorption. Therefore products produced from VESTAMID® L1670 BK 9.7504 maintain their dimensions in environments with varying humidity levels, while maintaining a high tenacity, a low coefficient of friction and good chemical resistance.
 

VESTAMID® L1670 BK 9.7504 is supplied as cylindrical granules, ready for processing in moisture-proof packaging.

 
Pigmentation may affect values.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM

Características de processamento/físicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez volumétrico, MVR 79 / * cm³/10min ISO 1133
Temperatura 230 / * °C -
Carga 2.16 / * kg -
Contração após a moldagem, paralelo 1.4 / * % ISO 294-4, 2577
Contração após a moldagem, perpendicular 0.7 / * % ISO 294-4, 2577
Propriedades mecânicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 1600 / - MPa ISO 527
Tensão no escoamento 47 / - MPa ISO 527
Deformação no escoamento 8 / - % ISO 527
Deformação nominal na ruptura >50 / - % ISO 527
Resistência ao impacto Charpy , +23°C N / - kJ/m² ISO 179/1eU
Resistência ao impacto Charpy, -30°C N / - kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalhe, +23°C 3 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
Res. impacto Charpy c/entalhe, -30°C 5 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
Propriedades térmicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Temperatura de fusão, 10°C/min 178 / * °C ISO 11357-1/-3
Temp. de transição vítrea, 10°C/min 37 / * °C ISO 11357-1/-2
Temperatura de deflexão térmica, 1.80 MPa 50 / * °C ISO 75-1/-2
Temperatura de deflexão térmica, 0.45 MPa 120 / * °C ISO 75-1/-2
Temperatura de amolecimento Vicat, B 140 / * °C ISO 306
Coef. de expansão térmica linear, paralelo 150 / * E-6/K ISO 11359-1/-2
Flamabilidade a 1.5mm esp. nom. HB / * class IEC 60695-11-10
Espessuras do tubo de teste 1.6 / * mm -
Propriedades elétricasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Constante dielétrica, 100Hz 3.8 / - - IEC 62631-2-1
Constante dielétrica, 1MHz 2.2 / - - IEC 62631-2-1
Fator de dissipação dielétrica, 100Hz 450 / - E-4 IEC 62631-2-1
Fator de dissipação dielétrica, 1MHz 280 / - E-4 IEC 62631-2-1
Resistividade volumétrica específica 1E13 / - Ohm*m IEC 62631-3-1
Índice comparativo de linha de fuga 600 / - - IEC 60112
Outras propriedadesSeco / CondUnidadeMétodo de ensaio
Absorção de água 1.4 / * % Sim. to ISO 62
Absorção de umidade 0.7 / * % Sim. to ISO 62
Densidade 1010 / - kg/m³ ISO 1183
Características
Processamento
Extrusão cabo
Forma de entrega
Granulos, Negro
Características especiais
Estável a luz, Estável contra o calor
Características
Grau tribológico
Resistência Química
Resistência química geral
Disponibilidade regional
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.