Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® L2124 - PA12 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® L2124:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto
High viscosity, plasticized, heat and light stabilized PA12 Compound for extrusion

VESTAMID® L2124 NC is a plasticized, heat- and light- stabilized polyamide 12 compound for the extrusion of flexible tubing and hoses especially for oil and petrochemical applications.

Tubing according to DIN 73 378, Type: PA 12-PHL.

VESTAMID® L2124 NC is characterized by a high melt viscosity and good dimensional control during pipe extrusion.

Properties of compounds based on PA12 vary little with changing humidity due to low moisture absorption. Parts made of this semi-crystalline material are characterized by exceptional impact strength, low coefficient of friction and good chemical resistance.

Pigmentation may affect values.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM

Características de processamento/físicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez volumétrico, MVR 19 / * cm³/10min ISO 1133
Temperatura 275 / * °C -
Carga 5 / * kg -
Contração após a moldagem, paralelo 0.7 / * % ISO 294-4, 2577
Contração após a moldagem, perpendicular 1.6 / * % ISO 294-4, 2577
Propriedades mecânicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 400 / 350 MPa ISO 527
Tensão no escoamento 26 / 22 MPa ISO 527
Deformação no escoamento 31 / 27 % ISO 527
Deformação nominal na ruptura >50 / >50 % ISO 527
Módulo de tensão de fluência, 1h * / 350 MPa ISO 899-1
Módulo de tensão de fluência, 1000h * / 270 MPa ISO 899-1
Resistência ao impacto Charpy , +23°C N / - kJ/m² ISO 179/1eU
Resistência ao impacto Charpy, -30°C N / N kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalhe, +23°C 140 / N kJ/m² ISO 179/1eA
Res. impacto Charpy c/entalhe, -30°C 6 / 6 kJ/m² ISO 179/1eA
Type of failure C / C - -
Propriedades térmicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Temperatura de fusão, 10°C/min 169 / * °C ISO 11357-1/-3
Temperatura de deflexão térmica, 1.80 MPa 45 / * °C ISO 75-1/-2
Temperatura de deflexão térmica, 0.45 MPa 98 / * °C ISO 75-1/-2
Temperatura de amolecimento Vicat, B 125 / * °C ISO 306
Coef. de expansão térmica linear, paralelo 180 / * E-6/K ISO 11359-1/-2
Coef. de expansão térmica linear, perpend. 170 / * E-6/K ISO 11359-1/-2
Flamabilidade a 1.5mm esp. nom. HB / * class IEC 60695-11-10
Espessuras do tubo de teste 1.6 / * mm -
Propriedades elétricasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Constante dielétrica, 100Hz 12 / 16 - IEC 62631-2-1
Constante dielétrica, 1MHz 3.8 / 4.2 - IEC 62631-2-1
Fator de dissipação dielétrica, 100Hz 1600 / 1600 E-4 IEC 62631-2-1
Fator de dissipação dielétrica, 1MHz 1500 / 2000 E-4 IEC 62631-2-1
Resistividade volumétrica específica 1E10 / 2E9 Ohm*m IEC 62631-3-1
Resistividade superficial específica * / 1E12 Ohm IEC 62631-3-2
Resistência elétrica 32 / 27 kV/mm IEC 60243-1
Índice comparativo de linha de fuga 600 / 600 - IEC 60112
Outras propriedadesSeco / CondUnidadeMétodo de ensaio
Absorção de água 1.3 / * % Sim. to ISO 62
Absorção de umidade 0.5 / * % Sim. to ISO 62
Densidade 1030 / 1040 kg/m³ ISO 1183
Diagrama
Viscosidade - taxa de cisalhamento , VESTAMID® L2124, PA12, Evonik
Tensão de cisalhamento - taxa de cisalhamento , VESTAMID® L2124, PA12, Evonik
Módulo de cisalhamento dinâmico - temperatura , VESTAMID® L2124 (dry), PA12, Evonik
Tensão - deformação , VESTAMID® L2124 (dry), PA12, Evonik
Módulo secante - deformação , VESTAMID® L2124 (dry), PA12, Evonik
Módulo de tração - temperatura , VESTAMID® L2124 (dry), PA12, Evonik
Características
Processamento
Moldagem por injeção, Extrusão de tubos, Extrusão de perfis, Outros tipos de extrusão
Forma de entrega
Granulos, Cor natural
Aditivos
Lubrificantes, Plastificante
Características especiais
Alto impacto., Estável a luz, Estabilidade a raios U.V./Intempéries, Estável contra o calor
Características
Grau tribológico
Resistência Química
Resistência química geral
Disponibilidade regional
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.