Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® LX9008 BK 9.7504 - PA12-I - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® LX9008 BK 9.7504:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto

High-viscosity, plasticizer-free extrusion compound with an extraordinary long-term heat resistance

VESTAMID® LX9008 BK 9.7504 is a plasticizer-free polyamide 12 compound, with an especially high long-term resistance under thermal load.

VESTAMID®  LX9008 BK 9.7504 is suitable to produce flexible tubes that are permanently exposed to higher temperatures, e.g., in the engine compartment of motor vehicles. Especially when used as diesel fuel lines they show significant advantages compared with standard grades, obvious in storage tests with diesel fuel.

The material absorbs only little moisture, thus leading to nearly unaffected dimensions and properties of the finished parts at changing ambient conditions.

Using VESTAMID® LX9008 BK 9.7504 for fuel lines one must pay attention to certain preconditions. The Technical Marketing Department gives you advice in selecting the suitable VESTAMID® compound.

Pigmentation may affect values.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 
 
FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM

Características de processamento/físicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Contração após a moldagem, paralelo 0.2 / * % ISO 294-4, 2577
Contração após a moldagem, perpendicular 1.9 / * % ISO 294-4, 2577
Propriedades mecânicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 1450 / 970 MPa ISO 527
Tensão no escoamento 41 / 39 MPa ISO 527
Deformação no escoamento 5 / 17 % ISO 527
Deformação nominal na ruptura >50 / >50 % ISO 527
Resistência ao impacto Charpy , +23°C N / N kJ/m² ISO 179/1eU
Resistência ao impacto Charpy, -30°C N / N kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalhe, +23°C 40 / 90 kJ/m² ISO 179/1eA
Res. impacto Charpy c/entalhe, -30°C 22 / 22 kJ/m² ISO 179/1eA
Type of failure C / C - -
Dureza Shore D 73 / * - ISO 7619-1
Propriedades térmicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Temperatura de fusão, 10°C/min 176 / * °C ISO 11357-1/-3
Temp. de transição vítrea, 10°C/min 47 / * °C ISO 11357-1/-2
Temperatura de deflexão térmica, 1.80 MPa 48 / * °C ISO 75-1/-2
Temperatura de deflexão térmica, 0.45 MPa 113 / * °C ISO 75-1/-2
Temperatura de amolecimento Vicat, B 145 / * °C ISO 306
Coef. de expansão térmica linear, paralelo 90.5 / * E-6/K ISO 11359-1/-2
Coef. de expansão térmica linear, perpend. 120 / * E-6/K ISO 11359-1/-2
Flamabilidade a 1.5mm esp. nom. HB / * class IEC 60695-11-10
Espessuras do tubo de teste 1.6 / * mm -
Propriedades elétricasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Constante dielétrica, 100Hz 3.7 / 4.7 - IEC 62631-2-1
Constante dielétrica, 1MHz 2.9 / 3.1 - IEC 62631-2-1
Fator de dissipação dielétrica, 100Hz 520 / 1040 E-4 IEC 62631-2-1
Fator de dissipação dielétrica, 1MHz 320 / 390 E-4 IEC 62631-2-1
Resistividade volumétrica específica 1E12 / 2.3E10 Ohm*m IEC 62631-3-1
Resistência elétrica 38 / 37 kV/mm IEC 60243-1
Índice comparativo de linha de fuga 600 / - - IEC 60112
Outras propriedadesSeco / CondUnidadeMétodo de ensaio
Absorção de água 1.4 / * % Sim. to ISO 62
Absorção de umidade 0.7 / * % Sim. to ISO 62
Densidade 1010 / - kg/m³ ISO 1183
Características
Processamento
Extrusão de tubos, Extrusão de perfis, Outros tipos de extrusão
Forma de entrega
Granulos, Negro
Características especiais
Alto impacto., Estável contra o calor
Disponibilidade regional
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.