Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® Terra HS22X-HI-H2 E70392 - PA610-I - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® Terra HS22X-HI-H2 E70392:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto

High-viscosity, heat-and light stabilized, Impact-modified polyamide 610 compound for extrusion

VESTAMID® Terra HS22X-HI-H2 BK E70392 is a polyamide 610 extrusion compound developed for the manufacturing of tubing systems with higher demands on heat resistance.

The melting point of VESTAMID® Terra HS22X-HI-H2 BK E70392 is being about 40°C higher than PA 11 and 12 compounds and allows higher peak temperatures in use. The compound is especially suitable for the extrusion of tubing systems that are exposed to high burst pressures at high service temperatures, e.g., hydraulic clutch lines.

The process temperature should be within a range of 240-270°C.

VESTAMID® Terra HS22X-HI-H2 BK E70392 is supplied as cylindrical, ready for processing, in moisture-proof bags.

VESTAMID® Terra is a group of new polyamides, the monomers for which are based entirely or partly on renewable raw materials.
VESTAMID® Terra HS is the polycondensation product of 1,6-hexamethylene diamine (H) and 1,10-decanedioic acid (sebacic acid-S). Because sebacic acid is derived from castor oil, VESTAMID® Terra HS is a material that is partly based on bio-based and renewable resources.


Pigmentation may affect values.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.TERRA.COM

Propriedades mecânicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 2000 / - MPa ISO 527
Tensão no escoamento 55 / - MPa ISO 527
Deformação no escoamento 4 / - % ISO 527
Deformação nominal na ruptura >50 / - % ISO 527
Resistência ao impacto Charpy , +23°C N / - kJ/m² ISO 179/1eU
Resistência ao impacto Charpy, -30°C N / - kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalhe, +23°C 18 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
Res. impacto Charpy c/entalhe, -30°C 12 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
Propriedades térmicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Temperatura de fusão, 10°C/min 222 / * °C ISO 11357-1/-3
Temp. de transição vítrea, 10°C/min 48 / * °C ISO 11357-1/-2
Temperatura de amolecimento Vicat, B 190 / * °C ISO 306
Outras propriedadesSeco / CondUnidadeMétodo de ensaio
Densidade 1060 / - kg/m³ ISO 1183
Características
Processamento
Extrusão de tubos, Extrusão de perfis, Outros tipos de extrusão
Forma de entrega
Granulos, Granulado, Negro
Características especiais
Alto impacto., Estável a luz, Estável contra o calor
Certifications
Contém recursos renováveis
Disponibilidade regional
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com