Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® E62-S1 - TPA - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® E62-S1:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto
Heat-stabilized compound based on polyamide 12 elastomer for molding of sport shoe soles

VESTAMID® E62-S1 is a PA 12 elastomer consisting of PA 12 segments and softening segments. The material is free of volatile or migrating plasticizer.

The VESTAMID® E represent thermoplastic elastomers generically characterized as polyether block copolyamides (PEBA) consisting of PA 12 and polyether segments.

VESTAMID® E62-S1 is especially developed for sport shoe soles. It has good impact strength at low temperatures.

VESTAMID® E62-S1 is supplied as cylindrical pellets in moisture-proof packaging, ready for processing.
 
The process temperatures should be within a range of 190°C – 230°C.

Pigmentation may affect values.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

The values presented are typical or average values, they do not constitute a specification.



FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM
Características de processamento/físicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez volumétrico, MVR 20 / * cm³/10min ISO 1133
Temperatura 240 / * °C -
Carga 2.16 / * kg -
Contração após a moldagem, paralelo 0.8 / * % ISO 294-4, 2577
Contração após a moldagem, perpendicular 1.4 / * % ISO 294-4, 2577
Propriedades mecânicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 389 / - MPa ISO 527
Tensão no escoamento 23 / - MPa ISO 527
Deformação no escoamento 32 / - % ISO 527
Deformação nominal na ruptura >50 / - % ISO 527
Resistência ao impacto Charpy , +23°C N / - kJ/m² ISO 179/1eU
Resistência ao impacto Charpy, -30°C N / - kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalhe, +23°C 121 / - kJ/m² ISO 179/1eA
Res. impacto Charpy c/entalhe, -30°C 8 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
Dureza Shore D 61 / * - ISO 7619-1
Propriedades térmicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Temperatura de fusão, 10°C/min 172 / * °C ISO 11357-1/-3
Temp. de transição vítrea, 10°C/min 10 / * °C ISO 11357-1/-2
Temperatura de deflexão térmica, 1.80 MPa 45 / * °C ISO 75-1/-2
Temperatura de deflexão térmica, 0.45 MPa 100 / * °C ISO 75-1/-2
Temperatura de amolecimento Vicat, B 110 / * °C ISO 306
Propriedades elétricasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Constante dielétrica, 100Hz 9 / - - IEC 62631-2-1
Constante dielétrica, 1MHz 4 / - - IEC 62631-2-1
Fator de dissipação dielétrica, 100Hz 1000 / - E-4 IEC 62631-2-1
Fator de dissipação dielétrica, 1MHz 1200 / - E-4 IEC 62631-2-1
Resistividade volumétrica específica 2E10 / 2.5E9 Ohm*m IEC 62631-3-1
Outras propriedadesSeco / CondUnidadeMétodo de ensaio
Absorção de água 1.1 / * % Sim. to ISO 62
Absorção de umidade 0.5 / * % Sim. to ISO 62
Densidade 1030 / - kg/m³ ISO 1183
Produção de amostra para testeValorUnidadeMétodo de ensaio
ISO Dados
Moldagem por injeção, temperatura da massa 220 °C ISO 294
Moldagem por injeção, temperatura do molde 35 °C ISO 294
Moldagem por injeção, velocidade de injeção 200 mm/s ISO 294
Características
Processamento
Moldagem por injeção
Forma de entrega
Granulos
Características especiais
Estável contra o calor
Aplicaciones
Equipo deportivo
Disponibilidade regional
América do Norte, Europa, Ásia Pacífico, America Centra e do Sul, Oriente/África
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.