Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® L1930 NC - PA12-GD30 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® L1930 NC:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto

Milled glass fiber filled PA 12-Plastic resin for the injection molding

VESTAMID® L1930 NC is a heat stabilized, with 30% milled glass fiber-reinforced PA 12 compound suitable for injection molding of stiff, relatively warp free molded parts.

Due to the reinforcement moldings from this compound exhibit a high strength and rigidity. Because PA 12 absorbs only little water, the parts have a good dimensional stability and almost unaffected mechanical properties at changing ambient humidity.

Due to the reinforcement the shrinking of moldings is decreased compared with unreinforced compounds. Using specialty short glass fibers for the reinforcement of VESTAMID® L1930 NC the difference between longitudinal and transverse shrinkage relating to the flow direction of the melt is significantly lower than with common glass fiber-reinforced products. Therefore especially low-warpage precision parts can be molded.

As a semi-crystalline material VESTAMID® L1930 NC feature an outstanding chemical resistance, e.g., against fuels, oils and fats.

VESTAMID® L1930 NC is supplied as cylindrical pellets in moisture-proof packaging.

Pigmentation may affect values.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM

Características de processamento/físicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez volumétrico, MVR 24 / * cm³/10min ISO 1133
Temperatura 240 / * °C -
Carga 5 / * kg -
Contração após a moldagem, paralelo 0.7 / * % ISO 294-4, 2577
Contração após a moldagem, perpendicular 0.6 / * % ISO 294-4, 2577
Propriedades mecânicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 3740 / - MPa ISO 527
Tensão no escoamento 63 / - MPa ISO 527
Deformação no escoamento 4.5 / - % ISO 527
Deformação nominal na ruptura 12 / - % ISO 527
Resistência ao impacto Charpy , +23°C 89 / - kJ/m² ISO 179/1eU
Type of failure C / - - -
Resistência ao impacto Charpy, -30°C 65 / - kJ/m² ISO 179/1eU
Type of failure C / - - -
Res. impacto Charpy c/entalhe, +23°C 8 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
Res. impacto Charpy c/entalhe, -30°C 11 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
Propriedades térmicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Temperatura de fusão, 10°C/min 178 / * °C ISO 11357-1/-3
Temperatura de deflexão térmica, 1.80 MPa 130 / * °C ISO 75-1/-2
Temperatura de deflexão térmica, 0.45 MPa 170 / * °C ISO 75-1/-2
Temperatura de amolecimento Vicat, B 170 / * °C ISO 306
Coef. de expansão térmica linear, paralelo 50 / * E-6/K ISO 11359-1/-2
Coef. de expansão térmica linear, perpend. 50 / * E-6/K ISO 11359-1/-2
Flamabilidade a 1.5mm esp. nom. HB / * class IEC 60695-11-10
Espessuras do tubo de teste 1.5 / * mm -
Cartão Amarelo (yellow card) disponível sim / * - -
Flamabilidade a espessura h HB / * class IEC 60695-11-10
Espessuras do tubo de teste 0.8 / * mm -
Cartão Amarelo (yellow card) disponível sim / * - -
Propriedades elétricasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Constante dielétrica, 100Hz 4.1 / - - IEC 62631-2-1
Constante dielétrica, 1MHz 3.4 / - - IEC 62631-2-1
Fator de dissipação dielétrica, 100Hz 310 / - E-4 IEC 62631-2-1
Fator de dissipação dielétrica, 1MHz 240 / - E-4 IEC 62631-2-1
Resistividade volumétrica específica >1E13 / - Ohm*m IEC 62631-3-1
Índice comparativo de linha de fuga 600 / - - IEC 60112
Outras propriedadesSeco / CondUnidadeMétodo de ensaio
Absorção de água 1.1 / * % Sim. to ISO 62
Absorção de umidade 0.5 / * % Sim. to ISO 62
Densidade 1240 / - kg/m³ ISO 1183
Diagrama
Módulo de cisalhamento dinâmico - temperatura , VESTAMID® L1930 NC (dry), PA12-GD30, Evonik
Características
Processamento
Moldagem por injeção
Forma de entrega
Granulos, Cor natural
Aditivos
Lubrificantes
Características especiais
Estável contra o calor
Características
Baixa deformação
Resistência Química
Resistência química geral, Resistência à gordura, Resistência a óleos
Disponibilidade regional
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.