Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® X7166 - PA12 FR(30) - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® X7166:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto

Low viscosity, self-extinguishing polyamide 12 compound, free of halogen and phosphorus

VESTAMID® X7166 NC is a heat stabilized PA 12 compound containing a non-migrating flame retardant, free of halogen and phosphorus. Tested according to UL94, VESTAMID® X7166 complies with the flammability class V-2.
 
Due to the halogen- and phosphorus-free flame retardants, VESTAMID® X7166 is especially suitable for the electronic and cable industry. It can be used for injection molding as well as for wire extrusion coating.
 
VESTAMID® X7166 is supplied as cylindrical granules, ready for processing, in moisture-proof bags.

Due to the flame retardants, the melt temperature should not exceed 260°C. We recommend melt temperatures within a range of 210°C to 230°C.

The use of colorants may affect property values. 

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

The values presented are typical or average values, they do not constitute a specification.

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM

Características de processamento/físicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez volumétrico, MVR 108 / * cm³/10min ISO 1133
Temperatura 250 / * °C -
Carga 2.16 / * kg -
Contração após a moldagem, paralelo 0.7 / * % ISO 294-4, 2577
Contração após a moldagem, perpendicular 0.8 / * % ISO 294-4, 2577
Densidade do fundido 860 kg/m³ -
Condutividade térmica do fundido 0.2 W/(m K) -
Capacidade térmica específica do fundido 3000 J/(kg K) -
Propriedades mecânicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 1890 / - MPa ISO 527
Tensão no escoamento 47 / - MPa ISO 527
Deformação no escoamento 5.8 / - % ISO 527
Deformação nominal na ruptura 20 / - % ISO 527
Resistência ao impacto Charpy , +23°C 57 / - kJ/m² ISO 179/1eU
Type of failure C / - - -
Resistência ao impacto Charpy, -30°C 80 / - kJ/m² ISO 179/1eU
Type of failure C / - - -
Res. impacto Charpy c/entalhe, +23°C 3 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
Res. impacto Charpy c/entalhe, -30°C 5 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
Propriedades térmicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Temperatura de fusão, 10°C/min 178 / * °C ISO 11357-1/-3
Temp. de transição vítrea, 10°C/min 41 / * °C ISO 11357-1/-2
Temperatura de deflexão térmica, 1.80 MPa 50 / * °C ISO 75-1/-2
Temperatura de deflexão térmica, 0.45 MPa 140 / * °C ISO 75-1/-2
Temperatura de amolecimento Vicat, B 150 / * °C ISO 306
Flamabilidade a 1.5mm esp. nom. V-2 / * class IEC 60695-11-10
Espessuras do tubo de teste 1.6 / * mm -
Flamabilidade a espessura h V-2 / * class IEC 60695-11-10
Espessuras do tubo de teste 0.8 / * mm -
Cartão Amarelo (yellow card) disponível sim / * - -
Flamabilidade conforme índice de oxigênio 34 / * % ISO 4589-1/-2
Propriedades elétricasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Constante dielétrica, 1MHz 3.6 / - - IEC 62631-2-1
Fator de dissipação dielétrica, 1MHz 340 / - E-4 IEC 62631-2-1
Resistividade volumétrica específica 1E12 / - Ohm*m IEC 62631-3-1
Resistência elétrica 28 / - kV/mm IEC 60243-1
Índice comparativo de linha de fuga 600 / - - IEC 60112
Outras propriedadesSeco / CondUnidadeMétodo de ensaio
Absorção de água 1.3 / * % Sim. to ISO 62
Absorção de umidade 0.6 / * % Sim. to ISO 62
Densidade 1070 / - kg/m³ ISO 1183
Produção de amostra para testeValorUnidadeMétodo de ensaio
ISO Dados
Moldagem por injeção, temperatura da massa 220 °C ISO 294
Moldagem por injeção, temperatura do molde 80 °C ISO 294
Moldagem por injeção, velocidade de injeção 200 mm/s ISO 294
Moldagem por injeção, pressão de recalque 70 MPa ISO 294
Diagrama
Volume específico - temperatura (pvT) , VESTAMID® X7166, PA12 FR(30), Evonik
Características
Processamento
Moldagem por injeção, Extrusão de perfis, Extrusão cabo, Outros tipos de extrusão, Revestimento
Forma de entrega
Granulos, Cor natural
Características especiais
Retardante de chama, Sem halogéneo, Sem fósforo, Estável contra o calor
Aplicaciones
Elétrica e Eletrônica
Disponibilidade regional
América do Norte, Europa, Ásia Pacífico, America Centra e do Sul, Oriente/África
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.