Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® X7229 - PA12 FR(30) - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® X7229:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto
High viscosity, self-extinguishing PA12 compound, free of halogen and phosphorus

VESTAMID® X7229 NC is a heat-stabilized and plasticized PA 12 compound containing a non-migrating flame retardant, free of halogen and phosphorus. VESTAMID® X7229 NC complies with the requirements of FAR 25.853 or ABD 0031.

 

Due to the halogen- and phosphorus-free flame retardants, VESTAMID® X7229 NC is especially suitable for interior parts in aircrafts, railway vehicles and ships. It can be used for extrusion as well as for injection molding.

Due to the flame retardants, melt temperature should not exceed 260°C. We recommend melt temperatures of 210-230°C.

 

VESTAMID® X7229 NC is supplied as cylindrical pellets ready for processing in moisture-proof bags.

Pigmentation may affect values.


Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM
Características de processamento/físicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez volumétrico, MVR 26 / * cm³/10min ISO 1133
Temperatura 220 / * °C -
Carga 10 / * kg -
Contração após a moldagem, paralelo 0.6 / * % ISO 294-4, 2577
Contração após a moldagem, perpendicular 0.8 / * % ISO 294-4, 2577
Propriedades mecânicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 980 / - MPa ISO 527
Tensão no escoamento 36 / - MPa ISO 527
Deformação no escoamento 17 / - % ISO 527
Deformação nominal na ruptura >50 / - % ISO 527
Resistência ao impacto Charpy , +23°C N / - kJ/m² ISO 179/1eU
Resistência ao impacto Charpy, -30°C N / - kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalhe, +23°C 11 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
Res. impacto Charpy c/entalhe, -30°C 5 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
Propriedades térmicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Temperatura de fusão, 10°C/min 175 / * °C ISO 11357-1/-3
Temperatura de deflexão térmica, 1.80 MPa 40 / * °C ISO 75-1/-2
Temperatura de deflexão térmica, 0.45 MPa 130 / * °C ISO 75-1/-2
Temperatura de amolecimento Vicat, B 150 / * °C ISO 306
Coef. de expansão térmica linear, paralelo 80 / * E-6/K ISO 11359-1/-2
Flamabilidade a 1.5mm esp. nom. V-2 / * class IEC 60695-11-10
Espessuras do tubo de teste 1.6 / * mm -
Flamabilidade a espessura h V-2 / * class IEC 60695-11-10
Espessuras do tubo de teste 0.8 / * mm -
Flamabilidade conforme índice de oxigênio 24 / * % ISO 4589-1/-2
Propriedades elétricasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Constante dielétrica, 1MHz 5 / - - IEC 62631-2-1
Fator de dissipação dielétrica, 1MHz 1700 / - E-4 IEC 62631-2-1
Resistividade volumétrica específica 1E11 / - Ohm*m IEC 62631-3-1
Índice comparativo de linha de fuga 600 / - - IEC 60112
Outras propriedadesSeco / CondUnidadeMétodo de ensaio
Absorção de água 1.4 / * % Sim. to ISO 62
Absorção de umidade 0.6 / * % Sim. to ISO 62
Densidade 1060 / - kg/m³ ISO 1183
Características
Processamento
Moldagem por injeção, Extrusão de perfis, Outros tipos de extrusão
Forma de entrega
Granulos, Cor natural
Aditivos
Plastificante
Características especiais
Retardante de chama, Sem halogéneo, Sem fósforo, Estável contra o calor
Aplicaciones
Avião e aeroespacial
Disponibilidade regional
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.