Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® X7393 BK 9.7507 - PA12-I - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® X7393 BK 9.7507:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto

High viscosity, plasticized, impact modified, heat- and light stabilized polyamide 12 compound

VESTAMID® X7393 BK 9.7507 is high viscosity, plasticized, impact modified, heat- and light stabilized polyamide 12 compound for flexible tubing and hoses for the automobile industry according to DIN 73 378 and DIN 74 324,Type PA 12-PHLY.

Parts made of VESTAMID® X7393 BK 9.7507 are characterized by optimized cold temperature impact resistance for the extrusion of semi-rigid tubing with increased burst pressure resistance as well as exceptional low coefficient of friction and good chemical resistance. Properties of compounds based on Polyamide 12 vary little with changing humidity due to their low moisture absorption.

VESTAMID® X7393 BK 9.7507 is supplied as pellets, ready for use, in moisture-proof bags.

Pigmentation may affect values.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM

Características de processamento/físicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez volumétrico, MVR 8 / * cm³/10min ISO 1133
Temperatura 230 / * °C -
Carga 5 / * kg -
Contração após a moldagem, paralelo 0.8 / * % ISO 294-4, 2577
Contração após a moldagem, perpendicular 1.4 / * % ISO 294-4, 2577
Propriedades mecânicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 560 / 495 MPa ISO 527
Tensão no escoamento 31 / 28 MPa ISO 527
Deformação no escoamento 26 / 26 % ISO 527
Deformação nominal na ruptura >50 / >50 % ISO 527
Resistência ao impacto Charpy , +23°C N / N kJ/m² ISO 179/1eU
Resistência ao impacto Charpy, -30°C N / N kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalhe, +23°C 115 / 124 kJ/m² ISO 179/1eA
Res. impacto Charpy c/entalhe, -30°C 8 / 8 kJ/m² ISO 179/1eA
Type of failure C / C - -
Propriedades térmicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Temperatura de fusão, 10°C/min 173 / * °C ISO 11357-1/-3
Temp. de transição vítrea, 10°C/min 24 / * °C ISO 11357-1/-2
Temperatura de deflexão térmica, 1.80 MPa 45 / * °C ISO 75-1/-2
Temperatura de deflexão térmica, 0.45 MPa 115 / * °C ISO 75-1/-2
Temperatura de amolecimento Vicat, B 130 / * °C ISO 306
Coef. de expansão térmica linear, paralelo 140 / * E-6/K ISO 11359-1/-2
Coef. de expansão térmica linear, perpend. 140 / * E-6/K ISO 11359-1/-2
Flamabilidade a 1.5mm esp. nom. HB / * class IEC 60695-11-10
Espessuras do tubo de teste 1.6 / * mm -
Propriedades elétricasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Constante dielétrica, 100Hz 7 / - - IEC 62631-2-1
Constante dielétrica, 1MHz 4.2 / - - IEC 62631-2-1
Fator de dissipação dielétrica, 100Hz 1900 / - E-4 IEC 62631-2-1
Fator de dissipação dielétrica, 1MHz 1100 / - E-4 IEC 62631-2-1
Resistividade volumétrica específica 1E10 / - Ohm*m IEC 62631-3-1
Índice comparativo de linha de fuga 600 / - - IEC 60112
Outras propriedadesSeco / CondUnidadeMétodo de ensaio
Absorção de água 1.2 / * % Sim. to ISO 62
Absorção de umidade 0.6 / * % Sim. to ISO 62
Densidade 1020 / - kg/m³ ISO 1183
Diagrama
Tensão - deformação , VESTAMID® X7393 BK 9.7507 (dry), PA12-I, Evonik
Módulo secante - deformação , VESTAMID® X7393 BK 9.7507 (dry), PA12-I, Evonik
Módulo de tração - temperatura , VESTAMID® X7393 BK 9.7507 (dry), PA12-I, Evonik
Características
Processamento
Moldagem por injeção, Extrusão de tubos, Extrusão de perfis, Outros tipos de extrusão
Forma de entrega
Granulos, Negro
Aditivos
Lubrificantes, Plastificante
Características especiais
Alto impacto., Estável a luz, Estabilidade a raios U.V./Intempéries, Estável contra o calor
Características
Grau tribológico
Resistência Química
Resistência química geral
Aplicaciones
Automóvel
Disponibilidade regional
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com