Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Badaflex® UL TPE-S 90A FR1 - SEBS - Bada AG

Material Data Center offers the following functions for Badaflex® UL TPE-S 90A FR1:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Badaflex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Propriedades mecânicasValorUnidadeMétodo de ensaio
ISO Dados
Deformação permanente por compressão a 70°C, 24h 57 % ISO 815
Deformação permanente por compressão a 100°C, 24h 79 % ISO 815
Resistência ao rasgamento 25 kN/m ISO 34-1
Dureza Shore A 90 - ISO 7619-1
Other Standards[S]
Resistência à tração 13 MPa DIN 53504
Deformação na Ruptura TPE 550 % DIN 53504
S: These properties are reported by the producer according standards that are different to our defaults.
Propriedades térmicasValorUnidadeMétodo de ensaio
ISO Dados
Flamabilidade a espessura h V-0 class IEC 60695-11-10
Espessuras do tubo de teste 0.4 mm -
Cartão Amarelo (yellow card) disponível sim - -
Outras propriedadesValorUnidadeMétodo de ensaio
Densidade 1290 kg/m³ ISO 1183
Recomendação de processamento Moldagem por injeçãoValorUnidadeMétodo de ensaio
Pré-secagem - temperatura 60 - 70 °C -
Pré-secagem - tempo 2 - 3 h -
Umidade do processamento ≤0.1 % -
Temperatura da massa 190 - 220 °C -
Temperatura do molde 20 - 40 °C -
Características
Processamento
Moldagem por injeção
Características especiais
Retardante de chama
Características
Boa adesão, Copolímero
Certifications
RoHS
Disponibilidade regional
América do Norte, Europa, Ásia Pacífico, America Centra e do Sul, Oriente/África
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.