Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of CP PRYME® Polycarbonate PC100RUL-18M BT Clear - PC - Chase Plastics

Material Data Center offers the following functions for CP PRYME® Polycarbonate PC100RUL-18M BT Clear:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other CP Pryme datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Características de processamento/físicasValorUnidadeMétodo de ensaio
ASTM Dados
Índice de fluidez, MFI 18 g/10min ASTM D 1238
Temperatura 300 °C -
Carga 1.2 kg -
Contração após a moldagem, paralelo 0.006 mm/mm ASTM D 955
Propriedades mecânicasValorUnidadeMétodo de ensaio
ISO Dados
Resistência ao impacto Charpy, +23°C N kJ/m² ISO 179/1eU
Resistência ao impacto Charpy, -30°C N kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalhe, +23°C 65 kJ/m² ISO 179/1eA
Res. impacto Charpy c/entalhe, -30°C 11 kJ/m² ISO 179/1eA
Resistência ao Impacto Izod, +23°C N kJ/m² ISO 180/1U
Impacto Izod com entalhe, +23°C 65 kJ/m² ISO 180/1A
ASTM Dados
Resistência à tração no escoamento 62.1 MPa ASTM D 638
Resistência à tração na ruptura 68.9 MPa ASTM D 638
Alongamento no escoamento 7 % ASTM D 638
Deformação na ruptura 130 % ASTM D 638
Módulo de flexão 2340 MPa ASTM D 790
Dureza Rockwell R118 - ASTM D 785
Resistência à abrasão (Taber) 10 mg/1000 cycles ASTM D 1044
Impacto Izod com entalhe, 1/8 in 690 J/m ASTM D 256
Resistência ao Impacto Izod, 1/8 in 3200 J/m ASTM D 256
Propriedades térmicasValorUnidadeMétodo de ensaio
ASTM Dados
UL94 flamabilidade HB - UL 94
DTUL @ 66 psi 138 °C ASTM D 648
DTUL @ 264 psi 129 °C ASTM D 648
Temperatura de amolecimento Vicat 154 °C ASTM D 1525
Condutividade térmica, estado sólido 0.036 W/(m K) ASTM C 177
Capacidade térmica específica 1260 J/(kg K) ASTM C 351
Propriedades ópticasValorUnidadeMétodo de ensaio
ASTM Dados
Haze 1 % ASTM D 1003
Transmitância luminosa 88 % ASTM D 1003
Índice de refração 1.59 - ASTM D 542
Outras propriedadesValorUnidadeMétodo de ensaio
Absorção de água, 24hr 0.15 % ASTM D 570
Absorção de água, equilíbrio 0.35 % ASTM D 570
Densidade 1200 kg/m³ ASTM D 792
Características
Forma de entrega
Granulos
Características especiais
Transparente
Disponibilidade regional
América do Norte
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.