Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of CELANEX® 5206HG - PET-GF15 - Celanese

Material Data Center offers the following functions for CELANEX® 5206HG:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Celanex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto
Celanex 5206HG is a 15% glass-filled polyester featuring super high surface gloss and high flow for long flow channels. A typical application is oven handles.

Flammability at thickness h (0.8 mm)HB-
Características de processamento/físicasValorUnidadeMétodo de ensaio
ISO Dados
Contração após a moldagem, paralelo 0.5 % ISO 294-4, 2577
Propriedades mecânicasValorUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 6400 MPa ISO 527
Tensão na ruptura 95 MPa ISO 527
Deformação na ruptura 1.8 % ISO 527
Res. impacto Charpy c/entalhe, +23°C 4.7 kJ/m² ISO 179/1eA
Propriedades térmicasValorUnidadeMétodo de ensaio
ISO Dados
Temperatura de fusão, 10°C/min 250 °C ISO 11357-1/-3
Temperatura de deflexão térmica, 1.80 MPa 180 °C ISO 75-1/-2
Temperatura de deflexão térmica, 0.45 MPa 220 °C ISO 75-1/-2
Flamabilidade a espessura h HB class IEC 60695-11-10
Espessuras do tubo de teste 0.8 mm -
Outras propriedadesValorUnidadeMétodo de ensaio
Densidade 1450 kg/m³ ISO 1183
Recomendação de processamento Moldagem por injeçãoValorUnidadeMétodo de ensaio
Temperatura da massa 270 - 300 °C -
Temperatura do molde 120 - 135 °C -
Características
Processamento
Moldagem por injeção
Forma de entrega
Granulos
Características
High Gloss
Outras informações
Moldagem por injeção
Rear Temperature 480-500 (250-260) deg F (deg C)
Center Temperature 490-510 (255-265) deg F (deg C)
Front Temperature 500-540 (260-270) deg F (deg C)
Nozzle Temperature 510-520 (265-275) deg F (deg C)
Melt Temperature 520-570 (270-300) deg F (deg C)
Mold Temperature 250-275 (120-135) deg F (deg C)
Back Pressure 0-25 psi
Screw Speed 50-75 rpm
Injection Speed Medium/Fast

Injection speed, injection pressure and holding pressure have to be optimized to the individual article geometry. To avoid material degradation during processing low back pressure and minimum screw speed have to be used. Overheating of the material has to be avoided. Up to 25% clean and dry regrind may be used.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com