Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of DOWLEX™ 2645 - (PE-LLD) - The Dow Chemical Company

Material Data Center offers the following functions for DOWLEX™ 2645:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Dowlex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Características de processamento/físicasValorUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez, MFI 0.85 g/10min ISO 1133
Temperatura 190 °C -
Carga 2.16 kg -
Propriedades térmicasValorUnidadeMétodo de ensaio
ISO Dados
Coef. de expansão térmica linear, paralelo 39 E-6/K ISO 11359-1/-2
ASTM Dados
Temperatura de amolecimento Vicat 107 °C ASTM D 1525
Propriedades ópticasValorUnidadeMétodo de ensaio
ISO Data
Haze 10 - ISO 14782
ASTM Dados
Brilho 59 - ASTM D 2457
Outras propriedadesValorUnidadeMétodo de ensaio
Densidade 918 kg/m³ ASTM D 792
Propriedades do filmeValorUnidadeMétodo de ensaio
ISO Dados
Tensão no escoamento, paralelo 7.5 MPa ISO 527-3
Tensão no escoamento, perpend. 6.3 MPa ISO 527-3
Tensão na ruptura, paralelo 39 MPa ISO 527-3
Tensão na ruptura, perpend. 40 MPa ISO 527-3
Deformação Máxima, paralelo 560 % ISO 527-3
Deformação Máxima, perpend. 670 % ISO 527-3
Queda de dardo A 480 g ISO 7765-1
Tipo de extrusão blown - -
Espessura de corpo de prova 0.05 mm -
Características
Processamento
Extrusão de filme soprado, Extrusão de laminas
Forma de entrega
Granulos, Branco
Características
Baixo odor
Certifications
Contacto com alimentos, Aprovação para contacto com alimentos10/2011, Food contact notification (FCN)
Disponibilidade regional
Europa, Oriente/África
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.