Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Eastar™ AN014-30 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Eastar™ AN014-30:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Eastar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto

Eastar™ Renew copolyester AN014-30 Natural is a high flow product that contains mold release. Other features include excellent appearance and clarity, good physical properties, chemical resistance, and ease of melt processing with an increase of 20-40% in flow length over copolyester AN004-30 Natural, as determined by spiral

flow testing. This high flow product is especially suited for those applications utilizing thin-walled intricate tools.

Eastar™ Renew copolyester AN014-30 Natural is approved for food contact and thereby under existing United States Food and Drug Administration (FDA) regulations, it may be used in food contact articles which comply with

the specifications and conditions of use in 21 CFR 177.1240.

Eastman Renew polymers have been certified by International Sustainability & Carbon Certification (ISCC), a global, independent agency for tracking sustainable content in a variety of industries. Renew polymers are produced with ISCC certified circular content by mass balance allocation.

Renew polymers enable a brand to reduce consumption of fossil feedstock-based plastics, achieve sustainability targets without compromise, and be a fast mover in a growing market for sustainable consumer products.

Características de processamento/físicasValorUnidadeMétodo de ensaio
ASTM Dados
Contração após a moldagem, paralelo 0.003 mm/mm ASTM D 955
Propriedades mecânicasValorUnidadeMétodo de ensaio
ASTM Dados
Resistência à tração no escoamento 50 MPa ASTM D 638
Resistência à tração na ruptura 43 MPa ASTM D 638
Alongamento no escoamento 5 % ASTM D 638
Deformação na ruptura 270 % ASTM D 638
Módulo de flexão 1900 MPa ASTM D 790
Dureza Rockwell R 107 - ASTM D 785
Impacto Izod com entalhe, 1/8 in 80 J/m ASTM D 256
Impacto Izod com entalhe, baixa temperatura 44 J/m ASTM D 256
Temperatura -40 °C -
Resistência ao Impacto Izod, 1/8 in N J/m ASTM D 256
Propriedades térmicasValorUnidadeMétodo de ensaio
ASTM Dados
DTUL @ 66 psi 73 °C ASTM D 648
DTUL @ 264 psi 66 °C ASTM D 648
Temperatura de amolecimento Vicat 86 °C ASTM D 1525
Propriedades ópticasValorUnidadeMétodo de ensaio
ASTM Dados
Haze 1 % ASTM D 1003
Transmitância luminosa 92 % ASTM D 1003
Outras propriedadesValorUnidadeMétodo de ensaio
Absorção de água, 24hr 0.15 % ASTM D 570
Densidade 1190 kg/m³ ASTM D 792
Recomendação de processamento ExtrusãoValorUnidadeMétodo de ensaio
Pré-secagem - temperatura 70 °C -
Pré-secagem - tempo 4 h -
Temperatura da massa 230 - 280 °C -
Temperatura do molde 15 - 30 °C -
Características
Processamento
Extrusão de perfis
Forma de entrega
Cor natural
Aditivos
Desmoldante
Características especiais
Transparente
Características
Copolímero
Resistência Química
Resistência química geral
Certifications
Contacto com alimentos, Aprovação de alimentos FDA 21 CFR, ISCC Plus
Aplicaciones
Embalaje
Disponibilidade regional
América do Norte, Europa, Ásia Pacífico, America Centra e do Sul, Oriente/África
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.