Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of HIPTEN® 22006 - (PE-LD) - HIP-Petrohemija

Material Data Center offers the following functions for HIPTEN® 22006:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Hipten datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Características de processamento/físicasValorUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez, MFI 0.6 g/10min ISO 1133
Temperatura 190 °C -
Carga 2.16 kg -
Propriedades mecânicasValorUnidadeMétodo de ensaio
ISO Dados
Tensão no escoamento 10 MPa ISO 527
Tensão na ruptura 16 MPa ISO 527
Dureza Shore D 46 - ISO 7619-1
Outras propriedadesValorUnidadeMétodo de ensaio
Densidade 922 kg/m³ ISO 1183
Propriedades do filmeValorUnidadeMétodo de ensaio
ISO Dados
Tensão no escoamento, perpend. 11 MPa ISO 527-3
Tensão na ruptura, paralelo 24 MPa ISO 527-3
Tensão na ruptura, perpend. 22 MPa ISO 527-3
Tipo de extrusão blown - -
Espessura de corpo de prova 0.04 mm -
Características
Processamento
Extrusão de filme soprado, Extrusão de tubos
Forma de entrega
Granulos
Disponibilidade regional
Europa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.