Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NIBLAN F20 - PBT-GF20 - Soredi S.p.a.

Material Data Center offers the following functions for NIBLAN F20:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Niblan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Características de processamento/físicasValorUnidadeMétodo de ensaio
ASTM Dados
Índice de fluidez, MFI 22 g/10min ASTM D 1238
Temperatura 250 °C -
Carga 2.16 kg -
Contração após a moldagem, paralelo 0.007 mm/mm ASTM D 955
Propriedades mecânicasValorUnidadeMétodo de ensaio
ASTM Dados
Resistência à tração na ruptura 110 MPa ASTM D 638
Módulo de flexão 6000 MPa ASTM D 790
Resistência à flexão 180 MPa ASTM D 790
Dureza Rockwell M 85 - ASTM D 785
Impacto Izod com entalhe, 1/8 in 57.6 J/m ASTM D 256
Impacto Izod com entalhe, baixa temperatura 43.2 J/m ASTM D 256
Temperatura -22 °C -
Propriedades térmicasValorUnidadeMétodo de ensaio
ISO Dados
Coef. de expansão térmica linear, perpend. 30 E-6/K ISO 11359-1/-2
ASTM Dados
UL94 flamabilidade HB - UL 94
Espessuras do tubo de teste 1.6 mm -
DTUL @ 264 psi 215 °C ASTM D 648
Temperatura de fusão 220 °C ASTM D 3418
Propriedades elétricasValorUnidadeMétodo de ensaio
ISO Dados
Constante dielétrica, 1MHz 3.7 - IEC 62631-2-1
Resistividade volumétrica específica >1E13 Ohm*m IEC 62631-3-1
Resistividade superficial específica >1E15 Ohm IEC 62631-3-2
Resistência elétrica 35 kV/mm IEC 60243-1
Outras propriedadesValorUnidadeMétodo de ensaio
Absorção de água, 24hr 0.4 % ASTM D 570
Densidade 1440 kg/m³ ASTM D 792
Características
Forma de entrega
Cor natural
Disponibilidade regional
Europa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.