Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Platamid® H 2513 Powder - PA* - ARKEMA

Material Data Center offers the following functions for Platamid® H 2513 Powder:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Platamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto
Platamid® H 2513 Powder
Copolyamide Hot Melt Adhesive / Textile Applications

Platamid® H 2513 Powder is a medium melt viscosity copolyamide adhesive powder for the production of fusible interlinings. 
Platamid® H 2513 Powder offers an excellent laundry resistance up to 60°C and an excellent resistance to all kind of steam treatment.

AVAILABLE GRADES
This product is available in different grain sizes:
- Platamid® H 2513 PA 80 (0-80 μm paste dot)
- Platamid® H 2513 PTA 170/20 (0-170 μm powder dot)
- Platamid® H 2513 PTA 170 (80-170 μm double dot)
PACKAGING
- Platamid® H 2513 PA 80 and Platamid® H 2513 PTA 170/20 are delivered in 20 kg sealed bags. 
- Platamid® H 2513 PTA 170 is delivered in 20 kg sealed bags and 500 kg sealed big bags (GRVS).
SHELF LIFE
Two years from the date of delivery. For any use above this limit, please refer to our technical services.
Características de processamento/físicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez volumétrico, MVR 30 / * cm³/10min ISO 1133
Temperatura 160 / * °C -
Carga 2.16 / * kg -
Propriedades térmicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Temperatura de fusão, 10°C/min 128 / * °C ISO 11357-1/-3
Características
Forma de entrega
Características
Copolímero
Disponibilidade regional
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.