Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Platamid® HX 2598 Pellets - PA* - ARKEMA

Material Data Center offers the following functions for Platamid® HX 2598 Pellets:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Platamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto
Platamid® HX 2598 Pellets
Copolyamide Hot Melt Adhesive / Extrusion Applications

Platamid® HX 2598 is a standard thermoplastic copolyamide hot melt adhesive available in pellet form. This medium melt viscosity grade is particularly suitable for manufacturing webs, nets, mono- and multi-filaments, and films by extrusion.Platamid® HX 2598 offers a very good adhesion to various polar substrates (thermoplastics, thermosets, metal, natural fibers, etc).  

AVAILABLE GRADES

This grade is available:

- undried with optical brightener (HX 2598 FA)

PACKAGING

Platamid® HX 2598 is delivered in 500 kg sealed big bags (GRVS).

SHELF LIFE

Two years from the date of delivery. For any use above this limit, please refer to our technical services.

Características de processamento/físicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez volumétrico, MVR 33 / * cm³/10min ISO 1133
Temperatura 160 / * °C -
Carga 2.16 / * kg -
Propriedades térmicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Temperatura de fusão, 10°C/min 143 / * °C ISO 11357-1/-3
Outras propriedadesSeco / CondUnidadeMétodo de ensaio
Densidade 1110 / 1110 kg/m³ ISO 1183
Características
Processamento
Extrusão de laminas
Forma de entrega
Granulos
Características
Boa adesão, Copolímero
Aplicaciones
Monofilament, Multifilament
Disponibilidade regional
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.