Características de processamento/físicas | Valor | Unidade | Método de ensaio |
Other Standards[S] |
Índice de fluidez, MFI |
20 |
g/10min |
DIN 53735 |
Temperatura |
220 |
°C |
- |
Carga |
10 |
kg |
- |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Propriedades mecânicas | Valor | Unidade | Método de ensaio |
ISO Dados |
Res. impacto Charpy c/entalhe, +23°C |
10 |
kJ/m² |
ISO 179/1eA |
Impacto Izod com entalhe, +23°C |
17 |
kJ/m² |
ISO 180/1A |
Other Standards[S] |
Módulo de tração |
2300 |
MPa |
DIN 53457 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Propriedades térmicas | Valor | Unidade | Método de ensaio |
Other Standards[S] |
Temperatura de amolecimento Vicat, B |
95 |
°C |
DIN 53460 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Outras propriedades | Valor | Unidade | Método de ensaio |
Other Standards[S] |
Densidade |
1060 |
kg/m³ |
DIN 53479 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Características
Forma de entrega
Negro
Disponibilidade regional
Europa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.