Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of RTP 2899 X 109568 A - TPO - RTP Company

Material Data Center offers the following functions for RTP 2899 X 109568 A:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other RTP datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Características de processamento/físicasValorUnidadeMétodo de ensaio
ASTM Dados
Contração após a moldagem, paralelo 0.0125 mm/mm ASTM D 955
Propriedades mecânicasValorUnidadeMétodo de ensaio
ASTM Dados
Módulo a 100% alongamento 3.45 MPa ASTM D 412
Dureza Shore A 88 - ASTM D 2240
Dureza Shore D 36 - ASTM D 2240
Resistência ao rasgamento 23.6 kN/m ASTM D 624
Impacto Izod com entalhe, 1/8 in N J/m ASTM D 256
Resistência à tração 4.14 MPa ASTM D 412
Propriedades térmicasValorUnidadeMétodo de ensaio
ASTM Dados
UL94 flamabilidade V-0 - UL 94
Espessuras do tubo de teste 1.59 mm -
Índice de oxigênio 29 % ASTM D 2863
Outras propriedadesValorUnidadeMétodo de ensaio
Densidade 1140 kg/m³ ASTM D 792
Moisture Content 0.03 % -
Recomendação de processamento Moldagem por injeçãoValorUnidadeMétodo de ensaio
Pré-secagem - temperatura 79.4 °C -
Pré-secagem - tempo 2 h -
Temperatura da massa 182 - 210 °C -
Temperatura do molde 15.6 - 65.6 °C -
Pressão de injeção 41.4 - 82.7 MPa -
Características
Processamento
Moldagem por injeção
Características especiais
Retardante de chama
Disponibilidade regional
América do Norte, Europa, Ásia Pacífico
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.