Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Topthane™ 2180 - TPU - Top Polymer Enterprise

Material Data Center offers the following functions for Topthane™ 2180:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Topthane datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto
For more detailed information, please read our
or contact our representatives in your region.
Propriedades mecânicasValorUnidadeMétodo de ensaio
ASTM Dados
Módulo a 100% alongamento 6.1 MPa ASTM D 412
Módulo a 300% alongamento 4.8 MPa ASTM D 412
Dureza Shore A 80 - ASTM D 2240
Resistência ao rasgamento 76.5 kN/m ASTM D 624
Resistência à tração na ruptura 36.7 MPa ASTM D 412
Deformação na ruptura 800 % ASTM D 412
Outras propriedadesValorUnidadeMétodo de ensaio
Densidade 1180 kg/m³ ASTM D 792
Recomendação de processamento Moldagem por injeçãoValorUnidadeMétodo de ensaio
Pré-secagem - temperatura 90 - 110 °C -
Pré-secagem - tempo 3 - 4 h -
Zona 1 170 - 180 °C -
Zona 2 180 - 200 °C -
Zona 3 190 - 210 °C -
Temperatura do bico 195 - 205 °C -
Velocidade de parafuso 50 - 80 rpm -
Pressão de injeção 50 - 100 MPa -
Contrapressão 0.3 - 0.6 MPa -
Pressão de recalque 30 - 60 MPa -
Características
Processamento
Moldagem por injeção
Forma de entrega
Granulos
Resistência Química
Resistência química geral, Resistência a óleos
Aplicaciones
Automóvel, Elétrica e Eletrônica, Equipo deportivo
Disponibilidade regional
Ásia Pacífico
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.