Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultrafuse ABS Fusion+ - ABS - BASF

Material Data Center offers the following functions for Ultrafuse ABS Fusion+:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ultrafuse datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Características de processamento/físicasValorUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez volumétrico, MVR 10 cm³/10min ISO 1133
Temperatura 250 °C -
Carga 5 kg -
Propriedades térmicasValorUnidadeMétodo de ensaio
ISO Dados
Temp. de transição vítrea, 10 °C/min 114 °C ISO 11357-1/-2
Temperatura de deflexão térmica, 1.80 MPa 71 °C ISO 75-1/-2
Temperatura de deflexão térmica , 0.45 MPa 91 °C ISO 75-1/-2
Outras propriedadesValorUnidadeMétodo de ensaio
Densidade 1070 kg/m³ ISO 1183
3D DataValorUnidadeMétodo de ensaio
Other Standards[S]
Módulo de tração, flat 1380 MPa ISO 527
Módulo de tração, upright 1110 MPa ISO 527
Resistência à tração, flat 29.5 MPa ISO 527
Resistência à tração, upright 17.9 MPa ISO 527
Deformação na ruptura, flat 10.9 % ISO 527
Deformação na ruptura, upright 2.1 % ISO 527
Módulo de flexão, flat 1410 MPa ISO 178
Módulo de flexão, on-edge 1130 MPa ISO 178
Módulo de flexão, upright 878 MPa ISO 178
Resistência à flexão, flat 48.3 MPa ISO 178
Resistência à flexão, on-edge 48.7 MPa ISO 178
Resistência à flexão, upright 23.1 MPa ISO 178
Resistência ao impacto Charpy, +23°C, flat 71.9 kJ/m² ISO 179/1eU
Resistência ao impacto Charpy, +23°C, on-edge 119 kJ/m² ISO 179/1eU
Resistência ao impacto Charpy, +23°C, upright 6.9 kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalhe, +23°C, flat 32 kJ/m² ISO 179/1eA
Res. impacto Charpy c/entalhe, +23°C, on-edge 41.9 kJ/m² ISO 179/1eA
Res. impacto Charpy c/entalhe, +23°C, upright 2.5 kJ/m² ISO 179/1eA
Resistência ao Impacto Izod, +23°C, flat 73.1 kJ/m² ISO 180/1U
Resistência ao Impacto Izod, +23°C, on-edge 131 kJ/m² ISO 180/1U
Resistência ao Impacto Izod, +23°C, upright 6.6 kJ/m² ISO 180/1U
Impacto Izod com entalhe, +23°C, flat 26.4 kJ/m² ISO 180/1A
Impacto Izod com entalhe, +23°C, on-edge 38.4 kJ/m² ISO 180/1A
Impacto Izod com entalhe, +23°C, upright 2.2 kJ/m² ISO 180/1A
S: These properties are reported by the producer according standards that are different to our defaults.
Características
Processamento
Additive Manufacturing
Forma de entrega
Monofilament
Características
Baixa deformação
Aplicaciones
Automóvel
Disponibilidade regional
América do Norte, Europa, America Centra e do Sul
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.