Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultramid® A3ZG7 OSI BK23273 - PA66-I-GF35 - BASF

Material Data Center offers the following functions for Ultramid® A3ZG7 OSI BK23273:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Ultramid A datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto
33% glass reinforced, heat stabilized, impact modified PA66 black with a combination of excellent impact resistance, toughness and strength.
Características de processamento/físicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Contração após a moldagem, paralelo 0.2 / * % ISO 294-4, 2577
Contração após a moldagem, perpendicular 0.9 / * % ISO 294-4, 2577
Propriedades mecânicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 9340 / - MPa ISO 527
Tensão na ruptura 147 / - MPa ISO 527
Deformação na ruptura 4.9 / - % ISO 527
Resistência ao impacto Charpy , +23°C 115 / - kJ/m² ISO 179/1eU
Resistência ao impacto Charpy, -30°C 117 / - kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalhe, +23°C 35 / - kJ/m² ISO 179/1eA
Res. impacto Charpy c/entalhe, -30°C 21 / - kJ/m² ISO 179/1eA
Propriedades térmicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Temperatura de deflexão térmica, 1.80 MPa 246 / * °C ISO 75-1/-2
Temperatura de deflexão térmica, 0.45 MPa 259 / * °C ISO 75-1/-2
Outras propriedadesSeco / CondUnidadeMétodo de ensaio
Densidade 1350 / - kg/m³ ISO 1183
Recomendação de processamento Moldagem por injeçãoValorUnidadeMétodo de ensaio
Pré-secagem - temperatura 60 °C -
Pré-secagem - tempo 1 - 2 h -
Umidade do processamento ≤0.2 % -
Temperatura da massa 288 - 305 °C -
Temperatura do molde 60 - 100 °C -
Diagrama
Tensão - deformação , Ultramid® A3ZG7 OSI BK23273 (dry), PA66-I-GF35, BASF
Tensão - deformação , Ultramid® A3ZG7 OSI BK23273 (cond.), PA66-I-GF35, BASF
Módulo secante - deformação , Ultramid® A3ZG7 OSI BK23273 (dry), PA66-I-GF35, BASF
Módulo secante - deformação , Ultramid® A3ZG7 OSI BK23273 (cond.), PA66-I-GF35, BASF
Características
Forma de entrega
Negro
Características especiais
Alto impacto.
Disponibilidade regional
América do Norte
Outras informações
Moldagem por injeção
Nylon 66 materials must be properly dried in order to provide parts with optimum strength and toughness. Nylon 66 materials are hygroscopic and will become degraded by excessive moisture during the injection molding process. For unopened bag/box, dry at 60 degC (140 degF) for 1-2 hours. For material exposed to the atmosphere, if additional drying is needed, dry at 66 degC (150 degF) or until the moisture level is between 0.04 - 0.20%.

Typical Profile
Melt Temperature: 288-305 degC (550-581 degF)
Mold Temperature: 60-100 degC (140-212 degF)
Injection Pressure: 35-125 MPa (5000-18000 psi)


Back Pressure: 0-0.35 MPa (0-50 psi)
Screw RPM 40-80
Screw Compression Ratio:3:1-4:1


Mold Temperatures
This product can be processed over a wide range of mold temperatures; however, for applications where aesthetics are critical, a mold surface temperature of 60-100 degC (140-212 degF) is recommended.

Pressures
Injection pressure controls the filling of the part and should be applied for 90% of ram travel. Packing pressure affects the final part and can be used effectively in controlling sink marks and shrinkage. It should be applied and maintained until the gate area is completely frozen off.

Fill Rate
Fast fill rates are recommended to ensure uniform melt delivery to the cavity and prevent premature freezing.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.