Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultrasint PA6 FR black - PA6 - BASF

Material Data Center offers the following functions for Ultrasint PA6 FR black:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ultrasint datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Características de processamento/físicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez volumétrico, MVR 10 / * cm³/10min ISO 1133
Temperatura 240 / * °C -
Carga 2.16 / * kg -
Propriedades térmicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Temperatura de fusão, 10°C/min 218 / * °C ISO 11357-1/-3
Temperatura de deflexão térmica, 1.80 MPa 113 / * °C ISO 75-1/-2
Temperatura de deflexão térmica , 0.45 MPa 207 / * °C ISO 75-1/-2
Temperatura de amolecimento Vicat , A 214 / * °C ISO 306
Temperatura de amolecimento Vicat, B 197 / * °C ISO 306
Flamabilidade a espessura h V-2 / * class IEC 60695-11-10
Espessuras do tubo de teste 0.8 / * mm -
Glow Wire Flammability Index (GWFI) 750 °C IEC 60695-2-12
GWFI - thickness tested (1) 1 mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (2) 1.6 mm -
Glow Wire Ignition Temperature (GWIT) 775 °C IEC 60695-2-13
GWIT - thickness tested (1) 1 mm -
Outras propriedadesSeco / CondUnidadeMétodo de ensaio
Densidade 1300 / - kg/m³ ISO 1183
Bulk density 550 kg/m³ -
3D DataSeco / CondUnidadeMétodo de ensaio
Other Standards[S]
Módulo de tração, flat 4750 / 2450 MPa ISO 527
Módulo de tração, upright 4500 / 2450 MPa ISO 527
Resistência à tração, flat 56 / 41 MPa ISO 527
Resistência à tração, upright 33 / 27 MPa ISO 527
Deformação na ruptura, flat 1.4 / 2.6 % ISO 527
Deformação na ruptura, upright 0.8 / 1.2 % ISO 527
Módulo de flexão, flat 4400 / 2000 MPa ISO 178
Módulo de flexão, upright 3850 / 2050 MPa ISO 178
Resistência ao impacto Charpy, +23°C, flat 4.8 / 7.4 kJ/m² ISO 179/1eU
Resistência ao impacto Charpy, +23°C, upright 2.5 / 3.6 kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalhe, +23°C, flat 1.3 / 1.6 kJ/m² ISO 179/1eA
Res. impacto Charpy c/entalhe, +23°C, upright 1 / 1.1 kJ/m² ISO 179/1eA
Resistência ao Impacto Izod, +23°C, flat 5 / 7 kJ/m² ISO 180/1U
Resistência ao Impacto Izod, +23°C, upright 3.4 / 3.8 kJ/m² ISO 180/1U
Impacto Izod com entalhe, +23°C, flat 1.8 / 2.1 kJ/m² ISO 180/1A
Impacto Izod com entalhe, +23°C, upright 1.5 / 1.5 kJ/m² ISO 180/1A
S: These properties are reported by the producer according standards that are different to our defaults.
Características
Processamento
Additive Manufacturing, Sinterização a laser
Forma de entrega
Pó, Negro
Características especiais
Retardante de chama
Características
Estabilidade térmica
Aplicaciones
Avião e aeroespacial, Automóvel, Elétrica e Eletrônica
Disponibilidade regional
Europa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com