Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® L-GF30 BK E70285 - PA12-GF30 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® L-GF30 BK E70285:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto
Glass-fiber reinforced, laser-weldable polyamide 12

VESTAMID®  L-GF30 BK E70285 is a glass fiber reinforced, heat-stabilized PA 12 compound with good IR laser transparency for injection molding. The material contains about 30% glass fibers, an ageing protective agent and processing aid for a fast and even form filling.

 

VESTAMID®  L-GF30 BK E70285 is laser-weldable by a diode-pumped or solid-state laser in the range of λ = 808–1064 nm. Using glass fiber reinforcement the strength and the heat deflection temperature are significantly increased.
 

Further advantages of VESTAMID® L-GF30 BK E70285 are the characteristic properties of polyamide 12 as low water absorption, good dimensional stability and almost the same properties at changing ambient humidity.

 

VESTAMID® L-GF30 BK E70285 is supplied as cylindrical pellets ready for processing in moisture-proof bags.

The use of colorants may change property values.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 
 

The values presented are typical or average values, they do not constitute a specification.

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM

Características de processamento/físicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez volumétrico, MVR 11 / * cm³/10min ISO 1133
Temperatura 250 / * °C -
Carga 5 / * kg -
Contração após a moldagem, paralelo 0.3 / * % ISO 294-4, 2577
Contração após a moldagem, perpendicular 0.9 / * % ISO 294-4, 2577
Propriedades mecânicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 6800 / - MPa ISO 527
Resistência ao impacto Charpy , +23°C 85 / - kJ/m² ISO 179/1eU
Type of failure C / - - -
Resistência ao impacto Charpy, -30°C 100 / - kJ/m² ISO 179/1eU
Type of failure C / - - -
Res. impacto Charpy c/entalhe, +23°C 23 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
Res. impacto Charpy c/entalhe, -30°C 21 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
Propriedades térmicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Temperatura de fusão, 10°C/min 178 / * °C ISO 11357-1/-3
Temperatura de deflexão térmica, 1.80 MPa 165 / * °C ISO 75-1/-2
Temperatura de deflexão térmica, 0.45 MPa 175 / * °C ISO 75-1/-2
Temperatura de amolecimento Vicat, B 175 / * °C ISO 306
Propriedades elétricasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Constante dielétrica, 100Hz 4 / - - IEC 62631-2-1
Constante dielétrica, 1MHz 3.2 / - - IEC 62631-2-1
Fator de dissipação dielétrica, 1MHz 290 / - E-4 IEC 62631-2-1
Resistividade volumétrica específica 7.2E12 / - Ohm*m IEC 62631-3-1
Resistência elétrica 48 / - kV/mm IEC 60243-1
Outras propriedadesSeco / CondUnidadeMétodo de ensaio
Absorção de água 1.1 / * % Sim. to ISO 62
Absorção de umidade 0.6 / * % Sim. to ISO 62
Densidade 1240 / - kg/m³ ISO 1183
Produção de amostra para testeValorUnidadeMétodo de ensaio
ISO Dados
Moldagem por injeção, temperatura da massa 250 °C ISO 294
Moldagem por injeção, temperatura do molde 80 °C ISO 294
Moldagem por injeção, velocidade de injeção 200 mm/s ISO 294
Características
Processamento
Moldagem por injeção
Forma de entrega
Granulos, Negro
Características especiais
Estável contra o calor
Características
Laser soldável, Soldável
Disponibilidade regional
América do Norte, Europa, Ásia Pacífico, America Centra e do Sul, Oriente/África
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.