Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® X7099 - PA612-GF20 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® X7099:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto

Especially developed for the production of plastic-rubber composites according to the Evonik Industries K K Process

VESTAMID® X7099 NC is a PA 612 resin especially developed for the production of plastic-rubber composites. 


Parts made from VESTAMID® X7099 can be, without the use of adhesives or adhesion promoters, covulcanized with rubbers, such as XNBR, HNBR, AEM or FPM ("direct-bonding to rubber").


As a partially crystalline resin VESTAMID® X7099 exhibits an outstanding chemical resistance, especially against fuels, oils and fats.


In comparison to resins based on PA 66 or PA 6 VESTAMID® X7099 has a distinctly lower water absorption.

VESTAMID® X7099 is supplied as cylindrical pellets ready for use in a moisture-proof packaging.

The use of colorants may affect property values. 

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

The values presented are typical or average values, they do not constitute a specification.

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM

Características de processamento/físicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Contração após a moldagem, paralelo 0.6 / * % ISO 294-4, 2577
Contração após a moldagem, perpendicular 0.9 / * % ISO 294-4, 2577
Propriedades mecânicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 5800 / - MPa ISO 527
Tensão no escoamento 125 / - MPa ISO 527
Deformação no escoamento 3.9 / - % ISO 527
Deformação nominal na ruptura 4.4 / - % ISO 527
Resistência ao impacto Charpy , +23°C 80 / - kJ/m² ISO 179/1eU
Type of failure C / - - -
Resistência ao impacto Charpy, -30°C 60 / - kJ/m² ISO 179/1eU
Type of failure C / - - -
Res. impacto Charpy c/entalhe, +23°C 10 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
Res. impacto Charpy c/entalhe, -30°C 7 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
Propriedades térmicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Temperatura de fusão, 10°C/min 215 / * °C ISO 11357-1/-3
Temperatura de deflexão térmica, 1.80 MPa 190 / * °C ISO 75-1/-2
Temperatura de deflexão térmica, 0.45 MPa 210 / * °C ISO 75-1/-2
Temperatura de amolecimento Vicat, B 205 / * °C ISO 306
Flamabilidade a 1.5mm esp. nom. HB / * class IEC 60695-11-10
Espessuras do tubo de teste 1.6 / * mm -
Propriedades elétricasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Constante dielétrica, 100Hz 4.4 / - - IEC 62631-2-1
Constante dielétrica, 1MHz 3.9 / - - IEC 62631-2-1
Fator de dissipação dielétrica, 100Hz 650 / - E-4 IEC 62631-2-1
Fator de dissipação dielétrica, 1MHz 430 / - E-4 IEC 62631-2-1
Resistividade volumétrica específica 1E12 / - Ohm*m IEC 62631-3-1
Outras propriedadesSeco / CondUnidadeMétodo de ensaio
Absorção de água 2 / * % Sim. to ISO 62
Absorção de umidade 0.8 / * % Sim. to ISO 62
Densidade 1200 / - kg/m³ ISO 1183
Produção de amostra para testeValorUnidadeMétodo de ensaio
ISO Dados
Moldagem por injeção, temperatura da massa 260 °C ISO 294
Moldagem por injeção, temperatura do molde 80 °C ISO 294
Moldagem por injeção, velocidade de injeção 200 mm/s ISO 294
Características
Processamento
Moldagem por injeção
Forma de entrega
Granulos, Cor natural
Características especiais
Estável contra o calor
Características
Boa adesão
Resistência Química
Resistência química geral, Resistência à gordura, Resistência a óleos
Disponibilidade regional
América do Norte, Europa, Ásia Pacífico, America Centra e do Sul, Oriente/África
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.