Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTODUR® GF30-FR3 BK V307168 - PBT-GF30 FR(17) - Evonik Operations GmbH

Material Data Center offers the following functions for VESTODUR® GF30-FR3 BK V307168:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestodur datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto

Glass fiber-reinforced and flame retardant polybutylene terephthalate compound

VESTODUR® GF30-FR3 BK V307168 is a glass fiber reinforced (with 30% glass fiber), semicrystalline thermoplastic compounds for injection molding, based on polybutylene terephthalate (PBT).

Test bars made of this compound are rated V-0, according UL94 by Underwriters Laboratories Inc., self-extinguishing and nondripping.
 

This compound is especially suitable for parts which are subjected to high mechanical and thermal loads and must have a very good flame-resistance.

The incorporated flame retardant is non-migrating and does not contain polybrominated diphenyl ethers. The additive has no corrosive effects on metal inserts or neighboring metal parts.

Therefore, the compounds are distinguished for moldings in the electrical and electronical industry. Laser marking with high contrasts is possible.

The compounds are supplied as cylindrical pellets in polyethylene packaging.

Pigmentation may affect values.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM 
OR VISIT OUR PRODUCT AT WWW.VESTODUR.COM

Características de processamento/físicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez volumétrico, MVR 12 / * cm³/10min ISO 1133
Temperatura 250 / * °C -
Carga 2.16 / * kg -
Contração após a moldagem, paralelo 0.3 / * % ISO 294-4, 2577
Contração após a moldagem, perpendicular 1.2 / * % ISO 294-4, 2577
Propriedades mecânicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 11000 / 10850 MPa ISO 527
Tensão na ruptura 140 / 125 MPa ISO 527
Deformação na ruptura 2 / 2 % ISO 527
Resistência ao impacto Charpy , +23°C 55 / 46 kJ/m² ISO 179/1eU
Type of failure C / C - -
Resistência ao impacto Charpy, -30°C 60 / 50 kJ/m² ISO 179/1eU
Type of failure C / C - -
Res. impacto Charpy c/entalhe, +23°C 10 / 8 kJ/m² ISO 179/1eA
Type of failure C / C - -
Res. impacto Charpy c/entalhe, -30°C 9 / 9 kJ/m² ISO 179/1eA
Type of failure C / C - -
Dureza Shore D 84 / * - ISO 7619-1
Propriedades térmicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Temperatura de fusão, 10°C/min 222 / * °C ISO 11357-1/-3
Temp. de transição vítrea, 10°C/min 44 / * °C ISO 11357-1/-2
Temperatura de deflexão térmica, 1.80 MPa 216 / * °C ISO 75-1/-2
Temperatura de deflexão térmica, 0.45 MPa 223 / * °C ISO 75-1/-2
Temperatura de amolecimento Vicat, B 213 / * °C ISO 306
Coef. de expansão térmica linear, paralelo 50 / * E-6/K ISO 11359-1/-2
Flamabilidade a 1.5mm esp. nom. V-0 / * class IEC 60695-11-10
Espessuras do tubo de teste 1.5 / * mm -
Flamabilidade a espessura h V-0 / * class IEC 60695-11-10
Espessuras do tubo de teste 0.8 / * mm -
Flamabilidade conforme índice de oxigênio 34 / * % ISO 4589-1/-2
Propriedades elétricasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Constante dielétrica, 100Hz 4.1 / - - IEC 62631-2-1
Constante dielétrica, 1MHz 4.4 / - - IEC 62631-2-1
Fator de dissipação dielétrica, 100Hz 30 / - E-4 IEC 62631-2-1
Fator de dissipação dielétrica, 1MHz 150 / - E-4 IEC 62631-2-1
Resistividade volumétrica específica 1E12 / - Ohm*m IEC 62631-3-1
Outras propriedadesSeco / CondUnidadeMétodo de ensaio
Absorção de água 0.4 / * % Sim. to ISO 62
Absorção de umidade 0.2 / * % Sim. to ISO 62
Densidade 1720 / - kg/m³ ISO 1183
Características
Processamento
Moldagem por injeção
Forma de entrega
Granulos, Negro
Características especiais
Retardante de chama
Características
Impressora a laser
Aplicaciones
Elétrica e Eletrônica
Disponibilidade regional
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.