Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Vydyne® 41H BK0677 - PA66 - Ascend

Material Data Center offers the following functions for Vydyne® 41H BK0677:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vydyne datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto
Vydyne 41H BK0677 is general-purpose, high impact-modified, heat stabilized PA66 resin. The product offers improved resistance to thermal degradation.
41H BK0677 is recognized for all the processing and property advantages inherent to PA66 with the addition of improved impact strength. This resin offers a well balanced combination of engineering properties characterized by high melt point, good surface lubricity, abrasion resistance and resistance to many chemicals, machine and motor oils, solvents and gasoline.
Características de processamento/físicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Contração após a moldagem, paralelo 1.8 / * % ISO 294-4, 2577
Contração após a moldagem, perpendicular 1.6 / * % ISO 294-4, 2577
Propriedades mecânicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 1790 / - MPa ISO 527
Tensão no escoamento 49 / - MPa ISO 527
Tensão na ruptura 49 / - MPa ISO 527
Deformação na ruptura 53 / - % ISO 527
Módulo de flexão, 23°C 1800 / - MPa ISO 178
Resistência à flexão 55 / - MPa ISO 178
Resistência ao impacto Charpy , +23°C N / - kJ/m² ISO 179/1eU
Resistência ao impacto Charpy, -30°C N / - kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalhe, +23°C 104 / - kJ/m² ISO 179/1eA
Res. impacto Charpy c/entalhe, -30°C 83 / - kJ/m² ISO 179/1eA
Impacto Izod com entalhe, +23°C 85 / - kJ/m² ISO 180/1A
Impacto Izod com entalhe 41 / - kJ/m² ISO 180/1A
Temperatura -40 °C -
Propriedades térmicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Temperatura de fusão, 10°C/min 262 / * °C ISO 11357-1/-3
Temperatura de deflexão térmica, 1.80 MPa 56 / * °C ISO 75-1/-2
Coef. de expansão térmica linear, paralelo 150 / * E-6/K ISO 11359-1/-2
Coef. de expansão térmica linear, perpend. 118 / * E-6/K ISO 11359-1/-2
Flamabilidade a 1.5mm esp. nom. HB / * class IEC 60695-11-10
Espessuras do tubo de teste 1.5 / * mm -
Flamabilidade a espessura h HB / * class IEC 60695-11-10
Espessuras do tubo de teste 0.8 / * mm -
Taxa de queima, FMVSS, espessura de 1mm 12 mm/min ISO 3795 (FMVSS 302)
Glow Wire Flammability Index (GWFI) 725 °C IEC 60695-2-12
GWFI - thickness tested (1) 0.75 mm -
Glow Wire Flammability Index (GWFI) 725 °C IEC 60695-2-12
GWFI - thickness tested (2) 1.5 mm -
Glow Wire Flammability Index (GWFI) 675 °C IEC 60695-2-12
GWFI - thickness tested (3) 3 mm -
Glow Wire Ignition Temperature (GWIT) 750 °C IEC 60695-2-13
GWIT - thickness tested (1) 0.75 mm -
Glow Wire Ignition Temperature (GWIT) 750 °C IEC 60695-2-13
GWIT - thickness tested (2) 1.5 mm -
Glow Wire Ignition Temperature (GWIT) 700 °C IEC 60695-2-13
GWIT - thickness tested (3) 3 mm -
ASTM Dados
UL94 flamabilidade HB - UL 94
Espessuras do tubo de teste 0.75 mm -
Propriedades elétricasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Resistividade volumétrica específica 1E8 / - Ohm*m IEC 62631-3-1
Resistência elétrica 14 / - kV/mm IEC 60243-1
Índice comparativo de linha de fuga 600 / - - IEC 60112
ASTM Dados
Resistência ao arco 330 / - s ASTM D 495
Outras propriedadesSeco / CondUnidadeMétodo de ensaio
Densidade 1070 / - kg/m³ ISO 1183
Recomendação de processamento ExtrusãoValorUnidadeMétodo de ensaio
Type of extrusion wire/cable - -
Pré-secagem - temperatura 80 °C -
Pré-secagem - tempo 4 h -
Temperatura da massa 285 - 305 °C -
Temperatura do molde 65 - 95 °C -
Zona 1 280 - 310 °C -
Zona 2 280 - 310 °C -
Zona 3 280 - 310 °C -
Temperatura do bico 280 - 310 °C -
Características
Processamento
Extrusão cabo, Outros tipos de extrusão
Forma de entrega
Granulos, Negro
Características especiais
Alto impacto., Estável contra o calor
Características
Resistência de derreta
Resistência Química
Resistência química geral, Resistência aos solventes, Resistência a óleos
Aplicaciones
Automóvel, Elétrica e Eletrônica, Polivalente
Disponibilidade regional
América do Norte, Europa, Ásia Pacífico
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.