Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Weezen HS 200 - PET - Selenis Portugal, S.A.

Material Data Center offers the following functions for Weezen HS 200:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Weezen datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Propriedades térmicasValorUnidadeMétodo de ensaio
Other Standards[S]
Temp. de transição vítrea 80 °C ASTM D 3418
S: These properties are reported by the producer according standards that are different to our defaults.
Outras propriedadesValorUnidadeMétodo de ensaio
Intrinsic Viscosity 0.8 dl/g -
Densidade 1290 kg/m³ ASTM D 792
Color L 64 - CIE
Color b 1 - CIE
Moisture Content 0.3 % -
Bulk Density 730 kg/m³ -
Recomendação de processamento ExtrusãoValorUnidadeMétodo de ensaio
Pré-secagem - temperatura 65 °C -
Pré-secagem - tempo 5 - 6 h -
Umidade do processamento ≤0.004 % -
Temperatura da massa 180 - 250 °C -
Características
Forma de entrega
Granulos
Características especiais
Transparente
Características
Amorfo, Baixo odor, Copolímero
Certifications
Contacto com alimentos, Aprovação para contacto com alimentos10/2011
Aplicaciones
Embalaje
Disponibilidade regional
América do Norte, Europa, America Centra e do Sul
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.