Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of CELCON® M90 - POM - Celanese

Material Data Center offers the following functions for CELCON® M90:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Celcon datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Любая форма использования представленной информации должна осуществляться на основании заявленных условий и с учетом отсутствия ответственности создателей системы.
Технологические и физические свойстваЗначениеЕдиницаСтандарт
Данные ISO
Показатель текучести расплава, ПТР 8 см³/10мин ISO 1133
Температура 190 °C -
Нагрузка 2.16 kg -
Усадка при литье, продольная 2.0 % ISO 294-4, 2577
Усадка при литье, поперечная 1.9 % ISO 294-4, 2577
Плотность расплава 1200 кг/м³ -
Теплопроводность расплава 0.155 W/(m K) -
Удельная теплоемкость расплава 2210 Дж/(кг K) -
Эффективный коэффициент теплопроводности 4.85E-8 м²/с -
Температура при извлечении из пресс-формы 140 °C -
Механические свойстваЗначениеЕдиницаСтандарт
Данные ISO
Модуль упругости при растяжении 2760 МПа ISO 527
Напряжение в точке текучести 65 МПа ISO 527
Удлинение в точке текучести 10 % ISO 527
Ударная вязкость по Шарпи, +23°C 188 кДж/м2 ISO 179/1eU
Ударная вязкость по Шарпи, -30°C 181 кДж/м2 ISO 179/1eU
Ударная вязкость по Шарпи с надрезом, +23°C 6 кДж/м2 ISO 179/1eA
Ударная вязкость по Шарпи с надрезом, -30°C 6 кДж/м2 ISO 179/1eA
Теплофизические свойстваЗначениеЕдиницаСтандарт
Данные ISO
Температура плавления, 10°C/мин 166 °C ISO 11357-1/-3
Температура изгиба под нагрузкой, 1.80 МПа 101 °C ISO 75-1/-2
Температура изгиба под нагрузкой, 0.45 МПа 158 °C ISO 75-1/-2
Коэффициент линейного теплового расширения, продольный 120 E-6/K ISO 11359-1/-2
Коэффициент линейного теплового расширения, поперечный 120 E-6/K ISO 11359-1/-2
Электрические свойстваЗначениеЕдиницаСтандарт
Данные ISO
Удельное объемное сопротивление 8E12 Ом*м IEC 62631-3-1
Удельное поверхностное сопротивление >1E15 Ом IEC 62631-3-2
Прочие свойстваЗначениеЕдиницаСтандарт
Водопоглощение 0.75 % Sim. to ISO 62
Поглощение влаги 0.2 % Sim. to ISO 62
Плотность 1410 кг/м³ ISO 1183
Рекомендации по переработке литьем под давлениемЗначениеЕдиницаСтандарт
Температура предварительной сушки 80 °C -
Время предварительной сушки 3 h -
Влажность переработки ≤0.35 % -
Температура расплава 182 - 199 °C -
Температура формы 82 - 93 °C -
Диаграммы
Напряжение - удлинение , CELCON® M90, POM, Celanese
Секущая модуля упругости - удлинение , CELCON® M90, POM, Celanese
Напряжение - удлинение (изохр.) 23°C, CELCON® M90, POM, Celanese
Модуль ползучести - время 23°C, CELCON® M90, POM, Celanese
Кривая ползучести 23°C, CELCON® M90, POM, Celanese
Напряжение - удлинение (изохр.) 40°C, CELCON® M90, POM, Celanese
Модуль ползучести - время 40°C, CELCON® M90, POM, Celanese
Кривая ползучести 40°C, CELCON® M90, POM, Celanese
Особые свойства и характеристики
Способы переработки
Литье под давлением, Пленочная экструзия, Экструзия профилированных изделий, Экструзия листа, Экструзия (прочие виды), Выдувное формование, Каландрирование
Вид поставки
Гранулы
Специальные характеристики
Сополимер
Доступность материала по регионам
Северная Америка, Европа, Страны Азии и Тихого океана, Латинская Америка, Ближний Восток и Африка
Другая текстовая информация
Литье под давлением
Drying is generally not required because Celcon® and Hostaform® acetal copolymers are not hydroscopic nor are they degraded by moisture during processing. Excessive moisture can lead to splay (silver streaking) in molded parts. For better uniformity in molding especially when using regrind or material that has been stored in containers open to the atmosphere, recommended drying conditions are 80 C (180 F) for 3hours. Desiccant hopper dryers are not required. Maximum water content = 0.35%
Standard reciprocating screw injection molding machines with a high compression screw (minimum 3:1 and preferably 4:1) and low back pressure (0.35 Mpa/50 PSI) are favored. Using a low compression screw (I.E. general purpose 2:1 compression ratio) can result in unmelted particles and poor melt homogeneity. Using a high back pressure to make up for a low compression ratio may lead to excessive shear heating and deterioration of the material.

Melt Temperature: Preferred range 182-199 C (360-390 F). Melt temperature should never exceed 230 C (450 F).

Mold Surface Temperature: Preferred range 82-93 C (180-200 F) especially with wall thickness less than 1.5 mm (0.060 in.). May require mold temperature as high as 120 C (250 F) to reproduce mold surface or to assure minimal molded in stress. Wall thickness greater than 3mm (1/8 in.) may use a cooler (65 C/150 F) mold surface temperature and wall thickness over 6mm (1/4 in.) may use a cold mold surface down to 25 C (80 F). In general, mold surface temperatures lower than 82 C (180 F) may hinder weld line formation and produce a hazy surface or a surface with flow lines, pits and other included defects that can hinder part performance.
Postprocessing conditioning and moisturizing are not required. It may be necessary to fixture large or complicated parts with varying wall thickness to prevent warpage while cooling to ambient temperature.
Экструзия пленки
Drying is generally not required because Celcon materials are not hydroscopic nor are they degraded by moisture during processing. Excessive moisture can cause surface defects on the extruded film. For better uniformity especially when using regrind or material that has been stored in containers open to the atmosphere, recommended drying conditions are 3 Hrs. at 80 C (180 F). Desiccant hopper dryers are not required. Max. moisture content = 0.35%.
Standard extruders with a length to diameter ratio of at least 20:1 are recommended. The screw should be a high compression ratio of at least 3:1 and preferably 4:1 to assure good melting and melt homogeneity. The design should be approximately 35% each for feed and metering sections with the remaining 30% as the transition zone.

Melt temperature: 160-220 C (320-430 F)
Postprocessing conditioning or moisturizing is not required.
Экструзия других изделий
Drying is generally not required because Celcon materials are not hydroscopic nor are they degraded by moisture during processing. Excessive moisture can cause surface defects. For better uniformity especially when using regrind or material that has been stored in containers open to the atmosphere, recommended drying is 3 hours at 80 C (180 F). Desiccant hopper dryers are not required. Max. moisture content = 0.35%
Standard extruders with a length to diameter ratio of at least 20:1 are recommended. The screw should be a high compression ratio of at least 3:1 and preferably 4:1 to assure good melting and uniform melt homogeneity. The design should be approximately 35% each for the feed and metering sections with the remaining 30% as transition zone.

Melt temperature 180-220 C (355-430F)
Postprocessing conditioning or moisturizing are not required. For thick walled sections (>3mm or 1/8 in.), annealing is recommended to reduce internal stresses.

Annealing temperature: 130-140 C (265-285 F)

Annealing time: 10 min/mm thickness
Экструзия профиля
Drying is generally not required because Celcon materials are not hydroscopic nor are they degraded by moisture during processing. Excessive moisture can cause surface defects on the extrusion. For better uniformity especially when using regrind or material that has been stored in containers open to the atmosphere, recommended drying conditions are 3 Hrs. at 80 C (180 F). Desiccant hopper dryers are not required. Max. moisture content = 0.035%.
Standard extruders with a length to diameter ratio of at least 20:1 are recommended. The screw should be a high compression ratio of at least 3:1 and preferably 4:1 to assure good melting and melt homogeneity. The design should be approximately 35% each for feed and metering sections with the remaining 30% as the transition zone.

Melt temperature: 180-220 C (360-430 F).
Postprocessing or moisturizing is not required. For thick walled extrusions (>3 mm or 1/8 in.), annealing is recommended to reduce internal stresses.

Annealing temperature: 130-140 C (265-285 F)
Annealing time: 10 min/mm thickness
Экструзия листа
Drying is generally not required because Celcon materials are not hydroscopic nor are they degraded by moisture during processing. Excessive moisture can lead to surface defects. For better uniformity in sheet extrusion especially when using regrind or material that has been stored in containers open to the atmosphere, recommended drying is 3 hours at 80 C (180 F). Desiccant hopper dryers are not required. Max. water content = 0.35%.
Standard extruders with a length to diameter ratio of at least 20:1 are recommended. The screw should be a high compression ratio (at least 3:1 and preferably 4:1) to assure good melting and uniform melt homogeneity. The screw design should be approximately 35% each for the feed and metering sections with the remaining 30% as the transition zone.

Melt temperature 180-190 C (355-375 F).
Postprocessing conditioning or moisturizing is not required. For thick walled sections (>3mm or 1/8 in.), annealing is recommended to reduce internal stresses.

Annealing temperature: 130-140 C (265-285 F)

Annealing time: 10 min/mm wall thickness
Литье методом раздува
Consult product information services.
Consult product information services.
Consult product information services.
Каландрование
Consult product information services.
Consult product information services.
Consult product information services.
Дискламация
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Создан: Источник: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.