Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Laperos - LCP - Polyplastics

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Laperos" in Material Data Center leads to the following information:

Tradename: Laperos
Family: LCP
Producer: Polyplastics
21 hits in the material database
1 hits in the literature database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
LAPEROS™ A130 LCP-GF30
LAPEROS™ A150 LCP-GF50
LAPEROS™ A230 LCP-CF30
LAPEROS™ A410 LCP-(GF+MD)50
LAPEROS™ E130G LCP-GF30
LAPEROS™ E130i LCP-GF30
LAPEROS™ E463i LCP-(MD+GF)40
LAPEROS™ E471i LCP-(GF+MD)35
LAPEROS™ E473i LCP-(MD+GF)30
LAPEROS™ E480i LCP-GF
LAPEROS™ E481i LCP-(MD+GF)45
LAPEROS™ GA130 LCP-GF30
LAPEROS™ HA475 LCP-(GF+MD)30
LAPEROS™ S135 LCP-GF35
LAPEROS™ S140M LCP-GF40
LAPEROS™ S150 LCP-GF50
LAPEROS™ S471 LCP-(MD+GF)45
LAPEROS™ S475 LCP-(MD+GF)30
LAPEROS™ E525T LCP-MD25
LAPEROS™ GA481 LCP-(MD+GF)45
LAPEROS™ S478 LCP-(MD+GF)40

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.