Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Platamid® HX 2507F Pellets - PA* - ARKEMA

Material Data Center offers the following functions for Platamid® HX 2507F Pellets:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Platamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Любая форма использования представленной информации должна осуществляться на основании заявленных условий и с учетом отсутствия ответственности создателей системы.
Описание продукта
Platamid® HX 2507F Pellets
Alcohol Soluble Copolyamides

Platamid® HX 2507F Alcohol Soluble Copolyamides comprises copolyamides of different structures, molecular weights and melting characteristics which are particularly well suited for coating solutions. The products offer good film forming properties, excellent abrasion resistance and good adhesion to both metallic and non-metallic surfaces. 

The main feature of all products us the ability to form stable solutions after dissolving in lower aliphatic alcohols, such as:
  • Methanol
  • Ethanol
  • Propanol / Isopropanol
  • Butanol / Isobutanol
  • or mixtures of these 

As well as in higher boiling alcohols, such as:
  • Benzyl alcohol
  • cyclohexanol
Aromatic hydrocarbons, like xylene, or SOLVESSO®, can be added at concentrations up to 20 to 30 parts by weight. These hydrocarbons do not interfere with dissolution, and improve storage stability. Solubility in conventional lacquer solvents such as ketones, esters or ethers is negligible.
All Platamid® grades are compatible in solution. This allows blending to achieve special effects. 


AVAILABLE GRADES

This grade is available:

Non-dried pellets („F“) with a maximum residual moisture content of ≤ 1.8 %

PACKAGING

In 25 kg paper bags with aluminium foil / polyethylene liners on 1000 kg pallets

SHELF LIFE

Two years from the date of delivery. For any use above this limit, please refer to our technical services.



Технологические и физические свойствасухой / кондЕдиницаСтандарт
Данные ISO
Показатель текучести расплава, ПТР 0.6 / * см³/10мин ISO 1133
Температура 190 / * °C -
Нагрузка 2.16 / * kg -
Теплофизические свойствасухой / кондЕдиницаСтандарт
Данные ISO
Температура плавления, 10°C/мин 155 / * °C ISO 11357-1/-3
Температура стеклования, 10°C/мин 115 / * °C ISO 11357-1/-2
Прочие свойствасухой / кондЕдиницаСтандарт
Водопоглощение 4.5 / * % Sim. to ISO 62
Плотность 992 / 992 кг/м³ ISO 1183
Особые свойства и характеристики
Способы переработки
Пленочная экструзия, Нанесение покрытий
Вид поставки
Гранулы
Специальные характеристики
Смеси полимерных материалов, Хорошая адгезия (приклеивание), Сополимер
Доступность материала по регионам
Дискламация
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Создан: Источник: www.materialdatacenter.com