Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Platamid® M 1757 Pellets - PA* - ARKEMA

Material Data Center offers the following functions for Platamid® M 1757 Pellets:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Platamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Любая форма использования представленной информации должна осуществляться на основании заявленных условий и с учетом отсутствия ответственности создателей системы.
Описание продукта
Platamid® M 1757 Pellets
Copolyamide Hot Melt Adhesive / Extrusion Applications

Platamid® M 1757 is a standard thermoplastic co-polyamide hot melt adhesive available in pellet form. This low to medium melt viscosity, fast re-crystallizing grade is particularly suitable for manufacturing webs, nets, mono- and multi-filaments, and films by extrusion.
Platamid®  M  1757offers a very good adhesion to various polar substrates (thermoplastics, thermosets, metal natural fibers, etc). 
Platamid®  M  1757has a very good dry cleaning resistance and washing resistance up to 60°C.

AVAILABLE GRADES
This product is available:
- Dried with optical brightener (M 1757 TA)
- Un-dried with optical brightener (M 1757 FA)
PACKAGING
- Platamid® M 1757 TA is delivered in 25 kg sealed bags.
- Platamid® M 1757 FA is delivered in 500 kg sealed big bags (GRVS).
These grades are ready to be processed.
SHELF LIFE
Two years from the date of delivery. For any use above this limit, please refer to our technical services.
Технологические и физические свойствасухой / кондЕдиницаСтандарт
Данные ISO
Показатель текучести расплава, ПТР 27 / * см³/10мин ISO 1133
Температура 160 / * °C -
Нагрузка 2.16 / * kg -
Теплофизические свойствасухой / кондЕдиницаСтандарт
Данные ISO
Температура плавления, 10°C/мин 106 / * °C ISO 11357-1/-3
Особые свойства и характеристики
Способы переработки
Пленочная экструзия
Вид поставки
Гранулы
Специальные характеристики
Хорошая адгезия (приклеивание), Сополимер
Применение
Моноволокно, Комплексная нить
Доступность материала по регионам
Дискламация
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Создан: Источник: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.