Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of PLEXIGLAS® Resist AG 100 - PMMA-I - Röhm GmbH

Material Data Center offers the following functions for PLEXIGLAS® Resist AG 100:
unit conversion, PDF datasheet print, comparison with other plastics, application examples, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Plexiglas datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Любая форма использования представленной информации должна осуществляться на основании заявленных условий и с учетом отсутствия ответственности создателей системы.
Описание продукта

Productprofil

PLEXIGLAS® Resist AG 100 is an amorphous thermoplastic molding compound, based on impact-modified polymethyl methacrylate (PMMA).

 

PLEXIGLAS® molding compounds have the following typical properties:

 

  • high weather resistance
  • excellent transmission and clarity
  • brilliant appearance
  • low weight – half the weight of glass
  • 100% recyclable – best life cycle assessment as compared with glass and PC
  • the pleasant feel and sound of the molded parts.

 

PLEXIGLAS® Resist AG 100 is characterized by the following special properties:

 

  • highest breaking strength and impact strength (30 times higher breaking strength than glass)
  • improved resistance to stress cracking
  • balanced property profile
  • clear reduction of reversible haze at very high and low temperatures
  • increased heat deflection temperature under load
  • AMECA listing, CAMPUS and moldflow data available

Application and approvals

PLEXIGLAS® Resist AG 100 has a balanced property profile and was specially developed for automotive glazing. This specialty molding compound meets all the relevant requirements for this field of application.
Apart from reducing the vehicle weight, injectionmolded glazing offers maximum freedom of design and functional integration, such as the integration of lighting or panel trim. An approval to ECE R43 is required for use as automotive glazing. The material has undergone and passed all tests in line with ECE R43.
The test report of the Materials Testing Agency in North Rhine-Westphalia is available for systems based on PLEXIGLAS® Resist AG 100 for rear side windows, roof and rear windows. Further details are available on request.

Processing

PLEXIGLAS® Resist AG 100 can be processed by injection molding of parts or by sheet extrusion and coextrusion. PLEXIGLAS® Resist AG 100 can be injection-molded on processing machines with a standard three-section screw for engineering thermoplastics in one-component or twocomponent processes.

Fabrication

Forming after extrusion
The forming conditions are the same as for extruded PLEXIGLAS®. The high optical quality of the surface after forming is also comparable. Predrying is not necessary in most cases. During heating, the material turns slightly white, but this disappears completely upon cooling.
Painting and screen printing
In principle, the same paints and lacquers can be used as for extruded PLEXIGLAS®. However, we recommend that you carry out preliminary tests in this case.
Coating
Surface coating, for example with polysiloxane systems, can be carried out by means of conventional processes.
Please send any questions on fabrication to automotive-glazing@evonik.com.

Physical Form / Packaging

PLEXIGLAS® Resist molding compounds are supplied as pellets of uniform size in 25kg polyethylene bags or 500kg boxes with PE lining. Other types of packaging are available on request.

Colors

PLEXIGLAS® Resist AG 100 for vehicle glazing is available in Clear-transparent (9V913). Beyond this, the transparent colors Green (6V176) and Gray (7V275) are available. Further colors on request: automotive-glazing@evonik.com

Sustainability

From production to recycling, the environmental impact of PLEXIGLAS® was tested in the life cycle assessment in accordance with ISO 14040ff and received a positive rating. In addition to its durability, PLEXIGLAS® offers convincing recyclability. It can be completely recycled by chemical conversion to its starting materials or directly reused.
Thus, in a study prepared by PE International AG, the environmental impacts during manufacture, application and disposal of automotive glazing made from PLEXIGLAS® were positively rated in comparison with reference systems (single-layer safety glass, laminated safety glass, PC). We will be pleased to provide more details on request.

Технологические и физические свойстваЗначениеЕдиницаСтандарт
Данные ISO
Показатель текучести расплава, ПТР 1.1 см³/10мин ISO 1133
Температура 230 °C -
Нагрузка 3.8 kg -
Механические свойстваЗначениеЕдиницаСтандарт
Данные ISO
Модуль упругости при растяжении 2200 МПа ISO 527
Напряжение в точке текучести 55 МПа ISO 527
Удлинение в точке текучести 5 % ISO 527
Номинальное удлинение при разрыве 45 % ISO 527
Ударная вязкость по Шарпи, +23°C 120 кДж/м2 ISO 179/1eU
Теплофизические свойстваЗначениеЕдиницаСтандарт
Данные ISO
Температура стеклования, 10°C/мин 112 °C ISO 11357-1/-2
Температура изгиба под нагрузкой, 1.80 МПа 100 °C ISO 75-1/-2
Температура изгиба под нагрузкой, 0.45 МПа 105 °C ISO 75-1/-2
Температура размягчения по Вика, B 105 °C ISO 306
Коэффициент линейного теплового расширения, продольный 110 E-6/K ISO 11359-1/-2
Класс горючести при номинальной толщине 1.5 мм HB класс IEC 60695-11-10
Толщина образца 1.6 мм -
желтая карточка (Yellow Card) да - -
Оптические свойстваЗначениеЕдиницаСтандарт
ISO Data
Коэффициент пропускания света 91 % ISO 13468-1, -2
Прочие свойстваЗначениеЕдиницаСтандарт
Водопоглощение 1.5 % Sim. to ISO 62
Поглощение влаги 0.5 % Sim. to ISO 62
Плотность 1160 кг/м³ ISO 1183
Параметры изготовления образцов для испытанийЗначениеЕдиницаСтандарт
Данные ISO
Литье под давлением, температура расплава 250 °C ISO 294
Литье под давлением, температура пресс-формы 82 °C ISO 294
Литье под давлением, скорость впрыска 195 мм/с ISO 294
Рекомендации по переработке литьем под давлениемЗначениеЕдиницаСтандарт
Температура предварительной сушки 70 - 80 °C -
Время предварительной сушки 3 - 4 h -
Температура расплава 235 - 270 °C -
Температура формы 60 - 80 °C -
Диаграммы
Вязкость - скорость сдвига , PLEXIGLAS® Resist AG 100, PMMA-I, Röhm
Касательное напряжение - скорость сдвига , PLEXIGLAS® Resist AG 100, PMMA-I, Röhm
Напряжение - удлинение (изохр.) 23°C, PLEXIGLAS® Resist AG 100, PMMA-I, Röhm
Модуль ползучести - время 23°C, PLEXIGLAS® Resist AG 100, PMMA-I, Röhm
Кривая ползучести 23°C, PLEXIGLAS® Resist AG 100, PMMA-I, Röhm
Модуль упругости при растяжении - температура , PLEXIGLAS® Resist AG 100, PMMA-I, Röhm
Особые свойства и характеристики
Способы переработки
Литье под давлением, Пленочная экструзия, Экструзия профилированных изделий, Экструзия листа, Экструзия (прочие виды), Термоформование
Вид поставки
Гранулы
Добавки
Добавка, улучшающая съем изделия с пресс-формы
Особые показатели
Ударопрочный или модифицированный к удару, Светостабилизироанный или стойкий к свету, Стабилизированный к УФ или погодостойкий, Прозрачный
Специальные характеристики
Аморфный
Химическая стойкость
Сопротивление растрескиванию агрессивной среде
Применение
Автомобилестроение
Доступность материала по регионам
Северная Америка, Европа, Страны Азии и Тихого океана, Латинская Америка, Ближний Восток и Африка
Другая текстовая информация
Литье под давлением
PREPROCESSING
Predrying temperature: 70 - 80°C
Predrying time in a desiccant-type drier: 3 - 4 h
PROCESSING
Melt temperature: 235 - 270°C
Mold temperature:60 - 80°C
Дискламация
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Создан: Источник: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.