Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Polyfort - PE, PP - LyondellBasell Industries

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Polyfort" in Material Data Center leads to the following information:

Tradename: Polyfort
Family: PE, PP
Producer: LyondellBasell Industries
193 hits in the material database
7 hits in the literature database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
POLYFORT® Aqualoy 125 PP-GX20
POLYFORT® Aqualoy 125M PP-GX20
POLYFORT® Aqualoy 135 PP
POLYFORT® Aqualoy 145 PP
POLYFORT® CB 1032 PP
POLYFORT® CB 3229 PP
POLYFORT® CFP 4611 PP-K11
POLYFORT® CFP 4623 PP-K20
POLYFORT® ComAlloy 130-3040B PP-GF
POLYFORT® ComAlloy E-10026 B PP
POLYFORT® ComAlloy E-14252B PP
POLYFORT® Comtuf 103 PP-GX
POLYFORT® E-13030B PP
POLYFORT® E-14526-31 PP-GX30
POLYFORT® E-15086-1B PP
POLYFORT® E-15937B PP
POLYFORT® E-16332 W PP-(GX+MX)40
POLYFORT® E-17162 PP
POLYFORT® E-17338 PP-K22
POLYFORT® FCB 1236-8555 PP-GF20
POLYFORT® FIPP 10 T PP-T10
POLYFORT® FIPP 15 GFC BM K2258 PP-GF15
POLYFORT® FIPP 20 T PP-T20
POLYFORT® FIPP 20 T LE K1731 PP-T20
POLYFORT® FIPP 20 T LE K1832 PP-T20
POLYFORT® FIPP 30 T K1005 PP-T30
POLYFORT® FIPP 30 TF PP-T30
POLYFORT® FIPP MKF 4025 PP-MX40
POLYFORT® FLP 3754 (PE-HD)
POLYFORT® FLP 674 (PE-HD)-GX36
POLYFORT® FPP 10 TFA K1741 PP-T10
POLYFORT® FPP 1006S PP-T20
POLYFORT® FPP 1007 PP-T40
POLYFORT® FPP 1007 F PP-T40
POLYFORT® FPP 1007E PP-T40
POLYFORT® FPP 1007X PP-T40
POLYFORT® FPP 1068-32 Black PP-MX40
POLYFORT® FPP 1082 PP-GX10
POLYFORT® FPP 1182 PP-T20
POLYFORT® FPP 1182E PP-T20
POLYFORT® FPP 1200 PP-K40
POLYFORT® FPP 1200H PP-K40
POLYFORT® FPP 1200X PP-K40
POLYFORT® FPP 1220 PP-GX20
POLYFORT® FPP 1227 PP-K40
POLYFORT® FPP 1236 PP-GX20
POLYFORT® FPP 1236-2939 PP-GF20
POLYFORT® FPP 1237 PP-K20
POLYFORT® FPP 1239H PP-GX30
POLYFORT® FPP 1244 PP-MX40
POLYFORT® FPP 1245 PP-K20
POLYFORT® FPP 1245I PP-K20
POLYFORT® FPP 1245U PP-K20
POLYFORT® FPP 1272 PP-T40
POLYFORT® FPP 1285 PP-GF20
POLYFORT® FPP 1285H PP-GX20
POLYFORT® FPP 1285U PP-GX20
POLYFORT® FPP 1310 PP-P
POLYFORT® FPP 1383 PP-T30
POLYFORT® FPP 1427 PP-MX25
POLYFORT® FPP 1434 PP-P25
POLYFORT® FPP 1453 PP-K40
POLYFORT® FPP 1477 PP-MX20
POLYFORT® FPP 1488 PP-P20
POLYFORT® FPP 1512 PP-T10
POLYFORT® FPP 1512E PP-T10
POLYFORT® FPP 1602 PP-GX10
POLYFORT® FPP 1602U-3120 PP-GX10
POLYFORT® FPP 1603 PP-GX10
POLYFORT® FPP 1605 PP-GX10
POLYFORT® FPP 1606 PP-GX30
POLYFORT® FPP 1607 PP-T30
POLYFORT® FPP 1608 PP-P10
POLYFORT® FPP 1609 PP-P10
POLYFORT® FPP 1666 PP-T10
POLYFORT® FPP 1697HU PP
POLYFORT® FPP 1829 PP-GX40
POLYFORT® FPP 1829U PP-GX40
POLYFORT® FPP 1842 PP
POLYFORT® FPP 1908E PP-T20
POLYFORT® FPP 20 GB PP-GB20
POLYFORT® FPP 20 GFC PP-GF20
POLYFORT® FPP 20 GFC LE K1400 PP-GF20
POLYFORT® FPP 20 GFM HI PP-GF20
POLYFORT® FPP 20 T PP-T20
POLYFORT® FPP 20 TE PP-T20
POLYFORT® FPP 2067HU PP
POLYFORT® FPP 2121UM-31 PP
POLYFORT® FPP 2122UM-31 PP-T40
POLYFORT® FPP 2181HU PP
POLYFORT® FPP 22 T K1093 PP-T22
POLYFORT® FPP 22 T LE K1684 PP-MX22
POLYFORT® FPP 2388 PP-GX5
POLYFORT® FPP 2496 PP
POLYFORT® FPP 2661 PP
POLYFORT® FPP 2937 PP
POLYFORT® FPP 30 GFC PP-GF30
POLYFORT® FPP 30 GFC K1079 PP-GF30
POLYFORT® FPP 30 T UV LE PP-T30
POLYFORT® FPP 30 T WLB PP-T30
POLYFORT® FPP 30/10 GBGF PP-(GB+GF)40
POLYFORT® FPP 3063UV-3120 PP-GX30
POLYFORT® FPP 3078M PP-GX10
POLYFORT® FPP 3391 PP
POLYFORT® FPP 3443U PP-T40
POLYFORT® FPP 3452 PP-MX30
POLYFORT® FPP 3454F PP-T20
POLYFORT® FPP 3459 PP-GX30
POLYFORT® FPP 3460 PP-(GX+MX)40
POLYFORT® FPP 3707 PP-K20
POLYFORT® FPP 3708U PP-K20
POLYFORT® FPP 3710 PP-GX45
POLYFORT® FPP 3711 PP-K26
POLYFORT® FPP 3715 PP-GX15
POLYFORT® FPP 3716 PP-T12
POLYFORT® FPP 3717 PP-T40
POLYFORT® FPP 3718 PP-GF25
POLYFORT® FPP 3722U PP-K35
POLYFORT® FPP 3725 PP-GX40
POLYFORT® FPP 3727 PP-MX24
POLYFORT® FPP 3728 PP-GB30
POLYFORT® FPP 3752 PP-MX16
POLYFORT® FPP 3765 PP-MX44
POLYFORT® FPP 3787U PP-GX30
POLYFORT® FPP 3799 PP
POLYFORT® FPP 3804 PP-MX
POLYFORT® FPP 3805 PP-T40
POLYFORT® FPP 3810 PP-K20
POLYFORT® FPP 3811 PP-MX40
POLYFORT® FPP 40 GFC PP-GF40
POLYFORT® FPP 40 GFC HI PP-GF40
POLYFORT® FPP 40 T PP-T40
POLYFORT® FPP 40 T LE K1846 PP-T40
POLYFORT® FPP 4020 PP-MX20
POLYFORT® FPP 4040 PP-MX40
POLYFORT® FPP 4529 PP-MX
POLYFORT® FPP 70 BS PP-Z70
POLYFORT® FPP 809 PP-T40
POLYFORT® FTP 3130H-01 PP
POLYFORT® FTP 3130HU-Colors PP
POLYFORT® FXP 1220U PP-GF20
POLYFORT® FXP 1227U PP-K20
POLYFORT® FXP 1245U PP-K40
POLYFORT® FXP 2600-3120 PP
POLYFORT® FXP 2779U PP-T20
POLYFORT® FXP 3000-3120 PP-GB30
POLYFORT® FXP 3748U-NGE PP-K20
POLYFORT® FXP 6630 (PA66+PP)-MX30
POLYFORT® PP 1329 PP
POLYFORT® PP 1329HU PP
POLYFORT® PP 1498HU PP
POLYFORT® PP 1544HU PP
POLYFORT® PP 1579H PP
POLYFORT® PP 1930UX PP
POLYFORT® PP 2173HU Toyota PP
POLYFORT® PP 2175HU Toyota PP
POLYFORT® PP 2175HU-31 PP
POLYFORT® PP 2268UX PP
POLYFORT® PP 2280H PP
POLYFORT® PP 2800 PP
POLYFORT® PP 2801 PP
POLYFORT® PP 2819 PP
POLYFORT® PP 2823 PP
POLYFORT® PP 2987C PP
POLYFORT® PP 3045 PP
POLYFORT® PP 3052UX PP
POLYFORT® PP 3153 PP
POLYFORT® PP 3701 PP
POLYFORT® PP 3702 PP
POLYFORT® PP 3719 PP
POLYFORT® PP 3720 PP
POLYFORT® PP 3726 PP
POLYFORT® PP 3730 PP
POLYFORT® PP 7001 PP
POLYFORT® PP 7031-01 PP
POLYFORT® PX 1040 PP
POLYFORT® PX 2561-01 PP
POLYFORT® PX 8242 PP
POLYFORT® Tempalloy 105 PP
POLYFORT® FIPP 10 T K2369 PP-T10
POLYFORT® FIPP 20 T K1742 PP-T20
POLYFORT® FPP 10 GFC PP-GF10
POLYFORT® FPP 1006U PP-T20
POLYFORT® FPP 1239 PP-GF31
POLYFORT® FPP 20 GFM HI HH PP-I-GF20
POLYFORT® FPP 2478 PP-MX25
POLYFORT® FPP 30 GFC K1079 LE PP-GF30
POLYFORT® FPP 3539 PP-GF15
POLYFORT® FPP 3551EU PP-GF20
POLYFORT® FPP 40 GFC LE PP-GF40
POLYFORT® FPP 40 GFC SHI PP-GF40
POLYFORT® FPP 40 T LE K2274 PP-T40
POLYFORT® FPP 40 TF PP-T40

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.